Abstract: The hot deformation behavior of the duplex structured Mg-9Li-5Al-2Sn-1.5Y alloy is investigated via hot compression tests in the temperature range of 200–350 °C and strain rate range of 0.001–1 s−1. The flow behavior of the Mg-9Li-5Al-2Sn-1.5Y alloy is defined by hyperbolic constitutive equation. The Zener–Hollomon parameter Z is used in the hyperbolic-sine-type equation to express the relationships between the peak stress, deformation temperature, and strain rate. Dynamic recovery and dynamic recrystallization are the main characteristics that affect deformation behaviors. The activation energy Q is calculated as 127.89 kJ/mol. Based on the dynamic materials model, the processing maps at strains of 0.6 and 0.8 are constructed, and the optimum processing parameters are determined as the temperature range of 320–350 °C and strain rate range of 0.001–0.007 s−1.
Source: Metals
Language: English
Open Access status: gold
Estimated APC paid: $3,137
OpenAlex ID: W4415812469
FWCI:
Cites: 32
Cited by:
Related to: