The Solidification Path of the Complex Metallic Al-Mn-Be Alloy
Year: 2010
Type: report
Abstract: The solidification paths of the Al 86.1 Mn 2.5 Be 11.4 and Al 84 Mn 5.1 Be 10.9 alloys, melt spun, cast into a copper mould and controlled cooled (during DSC) were investigated by means of light-optical microscopy (LOM), differential scanning calorimetry (DSC) combined with thermogravimetry (TG) or simultaneous thermal analysis (STA), scanning electron microscopy (SEM), transmission electron microscopy (TEM), Auger electron spectroscopy (AES) and the X-ray diffraction (XRD) line in Elletra Trieste, Italy.The constitutions of samples from both alloys were examined in all three states, i.e., after melt spinning, after casting into a copper mould and after differential scanning calorimetry.It was established that in the cast and controlled-cooled specimens the alloys consisted of an aluminium-rich α Al -matrix, and the Al 4 Mn and Be 4 AlMn phases.In the case of casting and DSC the primary crystallization began with the precipitation of the Be 4 AlMn phase, followed by what can most likely be characterized as a uni-variant binary eutectic reaction L → (Be 4 AlMn + Al 4 Mn).The solidification process continued with an invariant ternary eutectic reaction, where the remaining melt (L) formed the heterogeneous structure (α Al + Al 4 Mn + Be 4 AlMn) or a ternary eutectic.When extremely high cooling rates were employed, as is the case with melt-spinning, the constituting phases of both alloys were precipitated in a very small form and the Be 4 AlMn phase was completely absent in the form of primary polygonal particles and replaced by the icosahedral quasicrystalline phase or the i-phase.There was also no evidence of the Al 4 Mn phase.The distribution, size and shape of all the constituents in the melt-spun alloys also varied from the contact surface towards the free surface of the ribbons.The smallest constituents were established at the contact surface, measuring less than 0.1 μm, to 0.5 μm at the free surface.The grains of the aluminium-rich matrix had mean diameters of less than 20 μm, close to the free surface, down to 1 μm at the contact surface.
Institutions: University of Ljubljana, University of Maribor
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W65338580