Développement de méthodes d'échantillonnage de particules de poudre modifiées lors d'impressions par FSL de l'alliage de titane Ti64

Year: 2021
Type: dissertation
Abstract: Selective Laser Melting (SLM) is an Additive Manufacturing (AM) or 3D printing method that offers a variety of advantages compared to more conventional fabrication methods such as casting and machining. In fact, the printed parts can reach higher geometric complexity that allows to optimize the properties of the parts while minimizing their weight. Another advantage is the minimisation of the disposal of material compared to conventional methods. Indeed, after the SLM process, a large proportion of the powder that was not melted can be recycled for subsequent printings. However, the recycled powder can be modified during the SLM printing. Indeed, the scanning of the laser on the powder bed causes the generation of projected particles, or spatters, elsewhere on the powder bed. The local temperature elevation can also heat affect surrounding particles and modify their state. The effect of the various types of modified particles on the properties of the printed parts is not well known. It is important to thoroughly characterize each type of modified particles (amount, shape, size, color, chemical composition) in order to establish a relation between those particles and the effects on the properties of the printed parts. In this study, two sampling methods of spatters and heat affected particles near areas of the powder bed that was melted were developed in collaboration with Safran Tech and Tekna. The powder that was used during those printings is a Ti-6Al-4V ELI (grade 23) powder. The gathered samples allow the characterization of a large number of particles. Four types of spatters and one type of heat affected particle were identified. Among the spatter types, there is the unaffected and blown, the oxidized and colored, the large and spherical and the aggregates. The oxidized and colored spatters have an oxygen concentration at their surface (for an electron penetration depth of about 220 nm under the surface) of more than 8 wt% whereas the large and spherical spatters have an oxygen concentration at their surface of more than 5 wt%. The unaffected and blown spatters are oxidized similarly to the particles from the virgin powder and the oxygen concentration at the surface of the aggregates depend on the particles of the powder bed that contributed to the formation of the aggregate.
Author: Bissonnette, Julien
Language: French
Open Access status: green
OpenAlex ID: W6981063402
Cites: 87
Cited by:
Related to: 10