Year: 2025
Type: article
Abstract: A relationship between the microstructure of Ti5553 and its hydrogen absorption capacity was established for both additively and traditionally manufactured Ti5553.Hydrogen absorption rates during high pressure and temperature exposure are presented as well.Microstructural characterization using SEM revealed significant differences in phase precipitate morphology and phase fractions resulting from the manufacturing method and subsequent aging treatments employed.Hydrogen absorption experiments using a Sieverts apparatus revealed a strong positive correlation between secondary and grain boundary phase fractions and hydrogen absorption capacity.Electrochemical hydrogen charging followed by cross-sectional imaging showed that hydrogen ingress initiated primarily within the valleys of surface asperities, particularly those caused by partially fused powder particles in AM samples.Once inside the bulk material, a continuous layer along the grain boundary formed along prior grain boundaries acted as preferred diffusion pathways leading to hydride formation up to about 350 m in one sample.The results of the present work demonstrate key role precipitate morphology plays in the susceptibility of Ti5553 to hydrogen corrosion.Specifically, higher secondary (rod-like and acicular) phase fractions are associated with a greater hydrogen capacity, surface asperities can facilitate hydrogen ingress, and prior grain boundaries provide favorable diffusion pathways for hydrogen within the material when grain boundary forms along them.vi
Author: Shalloo, M [Lawrence Livermore National Laboratory]
Institution: Lawrence Livermore National Laboratory
Language: English
Subfield: Metals and Alloys
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W6982289984