Work

Toepassing van Kernmagnetische Resonantie Technieken in Ijzerrijke Alkali-Geactiveerde Materialen

Year: 2025
Type: dissertation
Abstract: Alkali-activated materials (AAMs) are sustainable alternatives to Portland cement, reducing CO2 emissions and promoting environmental sustainability. By using industrial by-products like fly ash and slags as precursors, AAMs reduce reliance on natural resources and minimize waste. This shift helps achieve carbon neutrality by lowering the carbon footprint of construction activities. AAMs synthesized from iron-rich precursors, such as non-ferrous metallurgical slags, have been found to exhibit mechanical properties comparable to Portland cement. Understanding the pore and molecular structures of these iron-rich AAMs is essential for optimizing their performance and durability. Nuclear magnetic resonance (NMR) techniques, such as low-field NMR relaxometry and solid-state NMR spectroscopy, are powerful tools for characterizing pore and molecular structures in materials with diamagnetic matrices. These methods are non-destructive and non-invasive, offering the ability to probe structures at the atomic level. However, characterizing samples containing iron with NMR techniques is challenging due to the magnetic properties of iron, which can interfere with the NMR signals and complicate the analysis. This limitation restricts the application of NMR techniques in studying iron-bearing samples, including iron-rich AAMs. In this work, we developed applications of low-field NMR relaxometry for iron-rich materials, aiding in understanding the iron oxidation state within the material and enabling in-situ monitoring of the Fe3+ leaching under acid attack. The iron-bearing AAMs were also characterized by solid-state 1D and 2D NMR experiments. Appropriate interpretation of the NMR results, together with complementary techniques, provided insight into the structural properties of these materials. The study began with low-field NMR investigations of low-iron-content alkali-activated materials (AAMs) with Fe wt% ≤ 4.0. A home-made variable NMR relaxometer was employed to explore how magnetic field strength and the forms of iron minerals impact NMR measurements. Samples containing Fe3O4 micropowder and Fe2O3 nanopowder exhibited severely underestimated NMR porosity and distorted pore size distributions due to the significant reduction in NMR signal intensity caused by their high magnetic susceptibility. The influence of magnetic susceptibility increases with magnetic field strength; therefore, it is recommended to use NMR relaxometry at a lower magnetic field for more accurate pore structure measurements. Additionally, the effect of Fe3+ introduced via ferric chloride water solution on T2 relaxation during the early stages (first three days) of curing has been investigated using NMR relaxometry at a magnetic field strength of 0.3 T. The results demonstrated that the introduced Fe3+ affected both the NMR signal by altering the surface relaxivity on the pore surfaces, and the pore structures, leading to an increase in pore sizes. A linear relationship between the surface relaxivity and the Fe3+ concentration was identified, providing a basis for converting relaxation times to pore sizes in porous materials with soluble iron. The study on the influence of Fe2+ and Fe3+ ions on the 1H relaxation in water solution indicated that the relaxation rate is linearly dependent on the concentration of these ions, with the contribution of Fe3+ ions being two orders of magnitude greater than that of Fe2+ ions. Building on this, the application of low-field NMR relaxometry to determine the redox ratio of iron in iron-rich materials was developed. The results were compared with data obtained from 57Fe Mössbauer spectroscopy, chemical titration, and theoretical calculations, demonstrating that the NMR method is a simple and reliable technique for determining the redox ratio of iron in iron-rich materials. Moreover, the non-destructive and non-invasive nature of NMR techniques provides the opportunity to in-situ monitor the dynamics of Fe3+ ion concentration in water solution. This capability was utilized to study the leaching kinetics of iron-rich AAMs under sulfuric acid attack. With the high temporal resolution of NMR measurements, a kinetic model tailored for a closed system was proposed to describe the leaching process. The molecular structure of iron-bearing AAMs was studied by 1D 29Si and 27Al solid-state NMR and 2D 27Al multi-quantum (MQ) NMR. 57Fe Mössbauer spectroscopy and Raman spectroscopy were employed to provide additional structural information. The paramagnetic effect on the NMR signals was discussed. The deconvolution results can quantify the silicate tetrahedra fractions since the linewidth of all silicate species widens equally. Results showed that after 7 days of curing, AAM synthesized from slag with Fe2+ has a less polymerized structure compared to AAM from slag with Fe3+. After 1 year of storage, the Fe2+-containing AAM showed the highest degree of polymerization with a chain-like structure. This Fe3+ coordination was likely contributed by a combination of tetrahedral and octahedral sites, with a higher fraction favoring octahedral coordination based on NMR analysis.
Source: Lirias
Author: Yu, Ziyou
Institution: KU Leuven
Language: English
Open Access status: green
OpenAlex ID: W6987652258
Cites: 254
Cited by:
Related to: 10