Fatigue behaviour and failure modes of monolithic CAD/CAM hybrid-ceramic and all-ceramic posterior crown restorations
Year: 2014
Type: dissertation
Abstract: The purpose of this in vitro study was to evaluate the mouth-motion-fatigue behaviour and failure modes of a novel CAD/CAM experimental hybrid-ceramic material and to compare it with two monolithic all-ceramic CAD/CAM materials (Vita Mark II and IPS e.max CAD) in a standardized molar crown model. The correlation between fracture load, cement thickness, crack length, and contact area size was also analysed. Resin-based composite dies (n = 54) were used as abutments for three different monolithic CAD/CAM fabricated crowns subdivided to one test group (experimental hybrid-ceramic) and two control groups (Vita Mark II and IPS e.max CAD) of 18 specimens each. All crowns were adhesively bonded using Variolink II (Ivoclar-Vivadent AG, Schaan, Liechtenstein) according to the manufacturer’s recommendations. 14 specimens from each group were exposed to a mouth-motion fatigue test using a fatigue simulator (Type N6C41/N6W26, Willytec, Munich, Germany) with loads of 198 N for 1.2 million cycles and temperature cycles of 5ºC and 55ºC. Subsequently, all specimens before (n = 4) and after (n = 14) fatigue were subjected to single load to failure testing in a universal testing machine (ZO10/TN2S, Zwick, Ulm, Germany). Statistical analysis of the fracture loads for the different materials was performed with Wilcoxon-Mann-Whitney test. A family-wise level of significance of 0.05 was obtained with the Bonferroni-Holm method. The novel experimental hybrid-ceramic crowns survived mouth-motion fatigue (100%) without any failures, while the control groups Vita Mark II and IPS e.max CAD crowns exhibited cracking with survival rates of 14.28% and 57.15%, respectively. The mean fracture loads before and after fatigue were as follows: experimental hybrid-ceramic (2060 ± 286 N, and 1883 ± 697 N), Vita Mark II (1580 ± 696 N, and 1313 ± 392 N), and IPS e.max CAD (2681 ± 886 N, and 2648 ± 739 N). Statistical analysis showed no significant influence of the fatigue cycling on the fracture load of the tested materials. No statistically significant influence of the cement thickness, contact area size, or crack length on the fracture load of tested materials was reported. Bulk fracture was the only failure mode reported for all tested monolithic CAD/CAM crowns. Monolithic CAD/CAM experimental hybrid-ceramic posterior crowns appeared to be fatigue resistant with fracture load results comparable to the monolithic CAD/CAM feldspathic (Vita Mark II) and lithium disilicate (IPS e.max CAD) ceramics. To confirm the results of the present study, long-term clinical studies are needed to be conducted.
Author: Bilkhair, Asma
Institution: University of Freiburg
Language: English
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: green
OpenAlex ID: W6991102190