"Virtuelle Passungsanalyse verschiedener Einstellungen des Marginal Gap anhand CAD/CAM gefertigter Zirkoniumdioxid-Einzelzahnrestaurationen - vor und nach der Zementierung"
Year: 2021
Type: dissertation
Abstract: Objective: The aim of this study was a virtual fit analysis of CAD/CAM (computer-aided design/computer-aided manufacturing) milled zirconia single crown copings with different settings of the marginal gap parameter with constant vertical and horizontal parameter and the influence of cementation by using two different luting agents on the final fit. Materials and Method: In this in-vitro investigation 60 CAD/CAM-milled zirconia copings were divided into three main groups (marginal gap 10 μm, -20 μm, -50 μm) each with 20 units. In order to evaluate the marginal gap parameter, each main group was subdivided into two subgroups (R_vor) and (F_vor) to determine after cementation the fit between the self-adhesive resin cement RelyX ™ Unicem 2 (R_zem) and the resin-modified glass ionomer cement GC FujiCem® 2 (F_zem) to compare it to before. An industrial noncontact scanner was used to digitize according it to a triple-scan protocol. For the measurement and calculation of the discrepancies, a CAD software was used, which enabled virtual three-dimensional surface analysis and two-dimensional virtual sectional analysis per unit. The marginal fit was illustrated by a marginal circular band and standardized measurement distances (n, z, xyz) of selected sections. Results: The “marginal gap 50 μm group” (R_vor/F_vor) reached on average the required marginal parameter. The “marginal gap 10 μm group” and “marginal gap 20μm group” (R_vor/F_vor) are marginally extended by 20 μm. After cementation, the caps cemented with GC FujiCem® 2 (F_zem) showed a greater spread than those cemented with RelyX ™ Unicem 2 (R_zem). Reduced marginal surface values were determined for the cemented marginal gap 50 μm group (R_zem/F_zem). The “marginal gap 10 μm group” and “marginal gap 20 μm group” (R_zem / F_zem) confirmed the fit deviation to the adapted state before cementation. By analysis, an increase in the absolute marginal discrepancy (xyz) was documented for all series of measurements. Conclusions: The mean marginal gap values were clinically acceptable in the present investigation. When using newer luting agents like RelyX™ Unicem 2 and GC FujiCem® 2, a marginal parameter configuration of 30 μm and 40 µm can be recommended. In the case of an increased fit of 50 µm, the crown copings drifted or rotated on the stump because of the improved flow properties and film thickness of the luting agents. In addition, the combination of 2D and 3D analysis can be useful in verifying the results to increase the value of the marginal fit of a restoration.
Author: Weiß, Christian Markus
Institution: Friedrich-Alexander-Universität Erlangen-Nürnberg
Language: German
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: green
OpenAlex ID: W7006854401