Abstract: In this dissertation three topics are presented: 1. the copolymerization of isobutylene (IB) and alloocimene (Allo), 2. the synthesis of PIB-based polyurethanes (PUs) using a PIB-diol, and 3. the design of a multi-jet needleless electrospinning device and the electrospinning of the synthesized PIB-based polymers.Di-and triblock copolymers were synthesized via carbocationic polymerization of IB and Allo with the AlCl 3 and EtAlCl 2 coinitiators with adventitious H 2 O as initiator, in methyl chloride (MeCl) at -95°C.The produced poly(Allo-IB-Allo) (AIBA) triblocks had good mechanical properties with 10-16 MPa tensile strength.The number average molar mass (M n ) of the products ranged from 120,000 to 250,000 g/mol with molar mass distributions (Ð) of 1.7-2.1.The reactions with EtAlCl 2 propagated slower than with AlCl 3 .The conversion of Allo was also slower, and it happened simultaneously with the IB reaction, which implies the formation of tapered blocks.A near-isothermal condition was achieved, during which chain transfer was minimal.PIB-diol (M n = 1850 g/mol, Ð = 1.59) was synthesized via carbocationic polymerization of IB with propylene oxide (PEpx) initiator/ TiCl 4 coinitiator and allyltrimethylsilane (ATMS) terminating agent, and subsequent functionalization with 2mercaptoethanol.Functionality of 2 for the PIB diol was confirmed by mass iv spectrometry.PIB-polyurethane (PIB-PU) elastomers were synthesized from dicyclohexylmethane 4,4'-diisocyanate and 1,4-butanediol in the hard segments and poly(hexamethylene carbonate) (PC) diol and polyisobutylene PIB-diol in the soft segments under solventless conditions with 30 minutes reaction time.The PU containing 30% PIB and 30% PC diol (PIB30-PC30-PU) retained 62.3 % of its 26.03 ±1.19 MPa tensile strength with no loss of elongation, displaying a stress-strain plot similar to that of the control PC-PU after hydrolytic stability testing.The control PC-PU retained only 27% of the initial 49.6 ±4.9 MPa tensile strength.A needleless electrospinning device capable of producing up to 50 jets at the same time was designed.Poly(ethylene oxide), poly(styrene-b-isobutylene-b-styrene) (SIBS), AIBA and PIB30-PC30-PU were electrospun with this device.The 4wt% (1100 mPa•s) PEO solution in water spun with 20-30 jets and created fibers of 100-500 nm diameter.Optimal conditions were achieved with an AIBA triblock (2016_07_29_AIBA_R2, M n = 235,000 g/mol, Ð = 1.9, Allo = 26 wt%) in 90/10 w/w CHCl 3 /C 2 Cl 4 as a 5 wt% solution containing PEG2000 in a 90/10 w/w AIBA/ PEG ratio and an triglyceride-based additive having 24 mPa•s dynamic viscosity.The AIBA fibers generated had an average size of 650±160 nm, much less that the 4-6 µm size achieved with single needle electrospinning.
Author: Kantor, Jozsef
Institution: University of Akron
Language: English
Subfield: Organic Chemistry
Field: Chemistry
Domain: Physical Sciences
Open Access status: green
Funder: National Science Foundation
OpenAlex ID: W7033997397