Abstract: While additive manufacture (AM) is an attractive technology for many areas of engineering, there \nare substantial barriers to its further industrialisation, one of which is the substandard surface \nroughness. Literature reviews showed there to be much interest in reducing the as built roughness \nthrough parameter optimisation, and various post processing options. One such post-processing \ntechnique is laser polishing (LP), sharing many of the benefits of AM (geometric freedom, waste-free \noperation). The literature reviews also highlighted a series of areas that needed specific attention to \nfacilitate the continued development of LP for AM metal parts, guiding the progress of this thesis. \nSpecific gaps identified were; how to effectively measure the surface roughness of AM parts, how to \nbest laser polish AM aluminium, and what effect the LP has on the material in terms of structure and \nmechanical properties. \nThis project started with developing a methodology to reliably and repeatably measure the surface \nroughness of AM metal parts. The developed methodology was benchmarked using AM aluminium \ntest parts, across a range of measurement devices. It was shown to be robust to changes in \nmeasurement device across a wide range of standard roughness parameters. This work also \nhighlights the need for greater understanding regarding the appropriate selection of filter nesting \nindex. Furthermore, the influence of various measurement and post-processing options on the \nmeasurement uncertainty have been quantified in terms of pointwise height discrepancies, and the \ninfluence on calculated roughness parameters. \nFollowing that, this project developed a novel LP strategy for AM aluminium, utilising multiple steps \ndesigned to sequentially ablate and smooth the surface. This was shown to significantly reduce the \nsurface roughness, with a dependency on the initial surface roughness. Minimum roughness values \nmeasured were 1.95 µm Sa, 18.83 µm Sp, 14.11 µm Sv, and 25.07 µm S10z. Maximum reductions \nfound were 87.4%, 87.4%, 81.7%, and 81.4% for the roughness parameters in turn. The LP strategy \nresulted in an increase in microhardness in the remelted region, with an associated increase in \nporosity just below this remelted layer. The maximum hardness after the final polishing step was \nmeasured to be 142 Hv0.005 (120 Hv0.005 bulk), while the near surface porosity was estimated to have \nrisen from 0.9% (bulk) to 4.5%. \nEvaluating the tensile properties showed mixed results, with LP giving increased, decreased, or no \nchange in values, and different effects depending on whether the samples had been stress relieved, \nor T6 tempered (peak hardened) prior to polishing. As built samples were found to have increased E \nand decreased Efail after LP, with the effect negated through the application of heat treatment. No \nchange in UTS was found due to LP in any condition This showed no \nsignificant change in fatigue strength due to the application of either LP or T6 tempering. Showing \nany benefit of the reduced surface roughness was offset by the increased surface hardness and \nporosity arising from the LP strategy used. \nIt is hoped that these results will facilitate the further industrialisation of AM aluminium through the \nimproved understanding of how to evaluate the surface roughness, with the smoothing potential of \nthe LP strategy opening avenues for high value, aesthetic components. Furthermore, the additional \ndata presented regarding the tensile and fatigue properties show there are no significant \ndetrimental effects of the LP strategy.
Author: Mason, Benjamin
Institution: Cardiff University
Language: English
Open Access status: green
OpenAlex ID: W7037070954
Cites: 120
Cited by:
Related to: 10