Year: 2015
Type: dissertation
Abstract: Electrodeposition is a cost-efficient and convenient method to prepare thin film materials on conductive substrates. The film morphology, composition and deposition rate can be easily controlled by changing the deposition conditions such as applied potential, current, temperature, agitation and bath composition. This PhD research investigated the electrodeposition of semiconductor materials: (1) electrodeposition of bismuth-tellurium and bismuth-antimony-tellurium thermoelectric materials from ethylene glycol solutions; and (2) electrodeposition of germanium from ionic liquids. Bismuth telluride and its derived alloys, (Bi1-xSbx)2(Se1-yTey)3 (0 < x,y<1), have the best thermoelectric properties at room temperature. In ethylene glycol, Bi(NO3)3, TeCl4 and SbCl3 have high solubilities up to 1 M which are more than 100 times higher than the solubility of Te(IV) ions in aqueous solutions. The most interesting finding is that the equilibrium alloy deposition can be achieved in chloride-free ethylene glycol solutions. This means the atomic ratio of bismuth to tellurium in the electrodeposited film is the same as the element ratio of [Bi(III)]/[Te(IV)] in the electrolyte. The film composition can be easily adjusted with the composition of the electrolyte. Removing Chloride ions also improves the film morphology and reduces the corrosiveness of the electrolyte. Mirror-like bismuth telluride films could be obtained from the chloride-free solutions. High deposition rate up to -3 A dm-2 was reached. Depending on the film composition, both p-type and n-type materials could be obtained. A maximum Seebeck coefficient of -120 µm V-1 was obtained. Preparation of multilayered Bi2Te3/(Bi1-xSbx)2Te3 thin films were studied for reducing the thermal conductivity and boosting the Seebeck coefficient. It was found that two different forms of antimony formed at different potentials. At lower overpotentials, the electrodeposited antimony is probably in a metastable ''explosive'' form that can rapidly change from amorphous into crystalline, and at higher overpotentials, crystalline antimony is electrodeposited. The deposition of bismuth-antimony and antimony-tellurium alloys followed the regular alloy deposition behavior. In a solution containing all three elements, ternary alloys with different compositions can be obtained and the composition depends on the deposition conditions. More antimony was present in the alloy if higher rotation speeds or higher overpotentials were applied. A pulsed potential was used to get multilayered structures and the layer thickness could be easily controlled by the pulse time. In theory, multilayered structures could reduce the thermal conductivity by phonon scattering at the interfaces of the layers. Electrodeposition of germanium has been performed in aqueous and organic solvents before. But due to the hydrogen evolution on germanium, only ultra thin films could be obtained from aqueous solutions and the current efficiency in organic solvent is extremely low. Ionic liquids are ideal solvents for germanium deposition because water can be easily removed and germanium tetrachloride (GeCl4) has a very high solubility in some ionic liquids. In this research, the germanium compound [GeCl4(BuIm)2], which is much less volatile than GeCl4, was synthesized and used in 1-butyl-1-methylpyrrolidinium dicyanamide ([BMP][DCA]). Black germanium films could be obtained. Only a small amount of oxygen impurity was found which could be due to the oxidation of germanium films in the air. This is a great improvement compared to the films deposited from solutions containing GeCl4. In those films, besides oxygen, chlorine and carbon impurities were always observed. However, electropolymerization of [DCA]- anions was observed on the cathode during deposition and the products were poorly conductive. To suppress the polymerization, [BMP]Cl was added and the deposition temperature was increased to 100 degreeC to make sure all [BMP]Cl was dissolved. The current density increase with increasing temperature. Temperatures above 100 degreeC still led to the polymerization of the [DCA]- anions. 1-Butyl-1-methylpyrrolidinium bis(trifluoromethylsulfonyl)imide [BMP][Tf2N] containing GeCl4 was used as electrolyte at elevated temperatures up to 180 degreeC. To prevent the evaporation of GeCl4, a pressure cell was designed and used. A high deposition rate of 6 µm h-1 was found at elevated temperatures due to the improved mass transport of the germanium compound and the kinetics of the reactions. The film morphology had also improved. Instead of black germanium films that always form at room temperature, metallic grey shiny germanium layers were obtained. Unfortunately, oxygen, carbon and chlorine impurities were found in the deposited films.
Source: Lirias
Author: Wu, Minxian
Institution: KU Leuven
Language: English
Subfield: Surfaces, Coatings and Films
Field: Materials Science
Domain: Physical Sciences
Keywords: electrodeposition, semiconductor thin films, non-aqueous electrolytes, ethylene glycol, ionic liquids, Bi2Te3, bismuth antimony telluride, thermoelectric materials, germanium, chloride-free electrolyte, alloy deposition, Seebeck coefficient, multilayer films, thermal conductivity reduction, film morphology
Open Access status: green
OpenAlex ID: W7046848899