Year: 2020
Type: conference-paper
Abstract: ZnO nanostructures are synthesize and fabricated successfully on glass substrates using a chemical bath deposition (CBD) technique. Then new design of \ncontinuous flow process has used at 0.05 M of zinc acetate hexahydrate [Zn (CH3COO)2.2H2O], 1.4 g of Hexamethylenetramine (CH2)6N4) and 250 mL of deionized water of the precursor solutions assisted by continuous wave laser irradiation at 532 nm laser wavelengths. The Ni and Pd, seed layers deposited and different growth time 20 and 25 min with same power. effects of different irradiation time 20 and 25 minutes. The x-ray diffraction (XRD) technique can exhibit well crystalline quality. Moreover, the FESEM images and energy dispersive x-ray spectra (EDX) shows uniformly distributed, dense ZnO \nnanostructures and the morphologies improved.
Authors: Lahewil, Abdulwahab Salem Zaroug, Ahmed, Naser Mahmoud, Azman, Nurul Zahirah Binti Noor
Language: English
Topic: ZnO doping and properties
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W7094719010