Year: 2023
Type: dissertation
Abstract: The sustainability of plastic packaging has been a focus in recent years for producing and consumer companies, which have been seeking to reduce plastic consumption and/or replace it with recyclable packaging. The multilayer plastic films usually used in food packaging are often rejected in the mechanical recycling waste streams, as they do not allow the separation of the different polymers that compose them, thus the use of compatibilizing additives to facilitate the miscibility of the different polymers has become an alternative. This research aimed to explore the effect of different concentrations (5-7%) of PCA-MA (compatibilizing additive based on polyolefin with maleic anhydride) on the properties, migration potential of two different multilayer packaging materials currently used for products meat products: PE/PE/ad/PA/ad/PE/PE and PE/ad/PA/EVOH/PA/ad/PE (PE: polyethylene; ad: adhesive; PA: polyamide; EVOH: ethylene vinyl alcohol) and evaluate the theoretical recyclability potential of the two multilayer films, using the RecyClass tool, as well as the post-industrial mechanical recycling of films without compatibilizer and with different concentrations of compatibilizer (5-7%). The incorporation of PCA-MA in the multilayer films resulted in a reduction in the crystallinity index and, consequently, a reduction in tensile strength, puncture resistance and water vapor barrier. The multilayer films presented values of total migration and specific migration of maleic anhydride below the limit of quantification of the methods used for simulants of aqueous and fatty foods. Therefore, they are within the specifications of the current legislation on materials for contact with food. Overall, although the incorporation of PCA-MA has resulted in some loss of packaging properties, this additive can be considered an attractive alternative to facilitate the recycling process of these complex materials. Multilayer films without compatibilizer were classified by RecyClass as non-recyclable materials. However, the use of the compatibilizer has shown to be promising for the recycling of these packages. The infrared spectra showed that the PA-MA-PE copolymer was created during the mixing, confirmed by the microscopy images, where the compatibilizer provided an adhesion between the mixing interface. The melting temperature of PE was stable during processing. However, the compatibilizer resulted in changes in the PA melting temperature of recycled film from PE/PE/ad/PA/ad/PE/PE packaging. Films with compatibilizer showed a significant increase in elongation at break compared to films without compatibilizer. These results confirm the strong efficiency of the PA-MA-PE ompatibilization, being an alternative for multilayer packaging of meat products to be recycled.
Author: Turriziani, Bruna Bonato
Institution: Instituto de Tecnologia de Alimentos
Language: Portuguese
Subfield: Polymers and Plastics
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
Awards: G1527757667, Plan of institutional development in research of the Institute of Food Technology - ITAL (PDIp), Multi-user equipment approved in grant 2017/50349-0: water vapor permeability system measurement, G29316538, Multi-user equipment approved in grant 2017/50349-0: oxygen permeability measurement system
OpenAlex ID: W7120466537