Resistência à degradação de restaurações em dentina sadia e afetada por cárie de dentes decíduos submetidas a desafios mecânico e cariogênico
Year: 2008
Type: dissertation
Abstract: This study aimed to investigate the resistance to degradation of resin modified glass ionomer cement (RMGIC) and adhesive/composite restorations on sound and caries-affected dentin of primary teeth subjected to carious challenge and load-cycling, by means of microtensile test and nanoleakage. Occlusal class I cavities were prepared on sixty sound exfoliated second primary molars. Half teeth were submitted to pH-cycling to induce artificial caries lesion. Teeth were randomly restored with one of the two materials: (1) a RMGIC (Vitremer®) and a (2) a total-etch adhesive system (Adper Single Bond 2®) followed by composite resin (Filtek Z100®). After storage in distilled water 37°C for 24 hours, sample from control groups followed to test procedures while the other ones were re-divided and submitted to two different aging methods: carious challenge (pH-cycling) and load-cycling (50 000 cycles, 90N, 3Hz). For testing, teeth were sectioned into about 1mm slabs, from which, one was separated for nanoleakage testing and the others were perpendicularly sectioned into 1mm2 beams that were tested to failure in tension in a universal testing machine. Data on microtensile bond strengths were registered in MPa and analyzed by ANOVA and Games-Howell multiple-comparisons tests (=0.05). Slabs meant for nanoleakage testing were coated with nail varnish except for the bonded interfaces, and immersed in ammoniacal AgNO3 for 24 hours in order to disclose nanometer-sized spaces and degradation signs within interfaces. After immersion in photodeveloping solution, bonded sections were prepared and observed under SEM using the backscattered electron mode. Nanoleakage patterns at interfaces were measured using Leica QWin, registered in m2 and analyzed by ANOVA and Tukey-Kramers multiple-comparisons tests. Vitremer bond strength was not affected by dentin condition (sound or affected). Conversely, Adper Single Bond 2® showed significantly lower bond strength values when bonded to caries-affected dentin. Load-cycling did not influence bond strength for both materials. While carious challenge resulted in a significant decrease in microtensile bond strengths of Adper Single Bond 2®, but did not for Vitremer restorations. The mixed failure pattern was predominant in all groups. Concerning nanoleakage, Vitremer® did not show difference in leakage pattern between sound and caries-affected dentins. In contrast, the adhesive Adper Single Bond 2®, presented greater leakage areas at affected dentin interfaces than sound ones. The cariogenic and mechanical challenges did not influence silver penetration for none of the materials and substrates. In conclusion, the caries-affected substrate and the cariogenic challenge negatively affected the behavior of the adhesive/composite restorations, but did not affect for RMGIC restorations.
Author: Marcela Marquezan
Institution: Universidade de São Paulo
Language: Portuguese
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: green
OpenAlex ID: W2135710037