Work

Reações de precipitação no estado sólido em um aço 25%Cr-5,5%Ni contendo 0,87% de nitrogênio

Year: 1995
Type: dissertation
Abstract: Nitrogen addition in stainless steels have shown to be beneficial to mechanical properties and corrosion resistance, mainly if nitrogen is in solid solution. In this work, it was studied a 25 wt %Cr 5.5 wt % Ni steel, which originally had ferritic-austenitic microstructure (DIN Werkstoff Nr. 1.4460), in which 0.87 wt% of nitrogen was added to become fully austenitic. The phase transformation that occurred between 700 and 1350°C were studied by employing several techniques such as optical microscopy, scanning electron microscopy, EDX microareas chemical analysis, x-ray diffraction, Vickers microhardness and magnetic measurements using a ferritoscope. The sample as-received presented an austenitic matrix with several (Cr, Fe)2N particles. Firstly, it was done various solution treatments between 1050 and 1350°C for 1 hour in order to choose the best temperature for solution treatment. Nitrides precipitation occurred in the lowest temperature meanwhile above 1300°C ferrite precipitated. As a result, the best condition for particles solution and absence of ferrite occurred at 1250°C for 1 hour. Afterwards the specimens were aged between 700 and 1100°C, for 90 seconds (salt bath) up to 100 hours. The first phase which precipitated was chromium nitride. This precipitation basically occurred in two maners: - Between 800 and 1500°C: discontinuos precipitation occurred predominantly ; - Above 1050 and bellow 800°C: continuous precipitation occurred predominantly. Ferrite precipitation occurred in long aging times, followed by sigma phase precipitation. A TTT diagram has been possible to be built up from the results of this work.
Language: Portuguese
Open Access status: green
OpenAlex ID: W2952967360
Cites:
Cited by: 2
Related to: 9