Avaliação da precisão da adaptação de próteses sobre implantes, fundidas em monobloco, com ligas de Ni-Cr e Co-Cr e em Ti cp, antes e após soldagem a laser e após a simulação da aplicação de cerâmica
Year: 2006
Type: dissertation
Abstract: The purpose of this study was to evaluate the precision of fit of three-element implant-retained and supported frameworks, cast in Ni-Cr- and Co-Cr alloys and commercially pure titanium (Cp Ti). The Sheffield´s test (EISENMAN, 1997) was used to analyze the marginal interfaces, and the readings executed in an optic microscope (Nikon, Japan). Two Master Conect AR (Conexão Sistemas de Prótese, Brazil) internal-hexagon implant systems were used. Data were submitted to analysis of variance (ANOVA) with complementary Tukey-Kramers test. Data analysis showed that: the interfaces, when analyzed as a one-piece casting and with both screws tightened, were better for the group cast in Ni-Cr alloy (25.00 ± 7.92μm), though not statistically different from the two other groups (Co-Cr: 54.23 ± 37.10μm e Cp Ti: 48.41 ± 26.69μm). In the single screw tightened test the three groups showed no statistical difference, with the following results, on the tightened side: Co-Cr: 35.01 ± 27.76μm, Ni-Cr: 20.13 ± 7.97μm, and Cp Ti: 22.28 ± 17.29μm, and on the opposite side: Co-Cr: 118.64 ± 91.48μm, Ni-Cr: 70.66 ± 20.88μm, and Cp Ti: 118.56 ± 51.35μm. On this same study, the one-piece castings were sectioned and laser welded. The laser welding was executed with the Desktop Laser (Dentaurum, Germany) machine. The Sheffield´s test was used to analyze the passive fit, and the readings executed in an optic microscope (Nikon). The procedure of sectioning the one-piece castings and its later laser welding presented statistically significant lower levels of misfit when the castings were analyzed with both screws tightened for the group cast in Co-Cr alloy (21.49 ± 9.08μm). For the other two groups, Ni-Cr alloy (13.10 ± 1.81μm) and Cp Ti (17.70 ± 11.70μm), results presented no statistically significant differences, though showed lower levels of marginal fit. In the single screw tightened test and readings made on the opposite side, only the group cast on Ni-Cr alloy (19.81 ± 7.36μm) didnt present statistically significant lower levels of misfit when compared to single-piece castings. The Co-Cr alloy (41.02 ± 26.15μm) and the Cp Ti (40.42 ± 27.14μm) groups showed statistically significant differences after laser welding. The reading on the screwed side detected that the three groups were statistically the same. Simulation of the porcelain firing cycles did not develop any significant differences on the analyzed interfaces under all readings and screw tightening conditions. The groups cast in Co-Cr alloy and Cp Ti, when analyzed with only one screw tightened and the readings executed on the opposite side, presented lower levels of misfit, being 26.42 ± 8.67μm, after simulation, when was 41.02 ± 26.15μm after laser welding for the first and, 40.42 ± 27.14μm and 28.05 ± 20.89μm, before and after, for the second, though not showing any statistically significant differences.
Author: Rodrigo Tiossi
Institution: Universidade de São Paulo
Language: Portuguese
Subfield: Oral Surgery
Field: Dentistry
Domain: Health Sciences
Open Access status: green
OpenAlex ID: W1536743410