Work

Blendas PBSA/PCL reforçadas com nanowhiskers de celulose enxertados com PCL

Year: 2013
Type: dissertation
Abstract: In this dissertation results of the study aimed to develop polymer blends composed of two biodegradable polymers, poly (butylene succinate - co - adipate) (PBSA) and aliphatic polyester polycaprolactone (PCL). The study developed the technology for the incorporation of cellulose nanowhiskers (NWC) grafted PCL (NWC - g - PCL), aiming to improve adherence nanowhisker / matrix, and improve mechanical properties of these polymers. The compositions used were 30PCL/70PBSA and 50PCL/50PBSA (in mass%), with 1, 3 and 5% of NWC - g - PCL. The blends and composites were prepared as films by evaporation of solvent chloroform (casting) and via extrusion and injection molding, and characterized their thermal, mechanical and morphological means of differential scanning calorimetry (DSC), thermogravimetric analysis (TGA) mechanical and thermodynamic analysis (DMTA), mechanical tests and scanning electron microscopy (SEM). The results obtained by analysis of infrared spectroscopy (IR) and X -ray diffraction (XRD) suggest the grafting of PCL chains in the NWC. The pure polymers in the form of films obtained by solvent evaporation, showed similar thermal stability with decomposition onset at 290°C and decomposition maximum at around 420°C. The films of the composites showed a decrease in thermal stability with increased levels NWC - g - PCL in the formulations. The DSC curves show two melting peaks and crystallization which indicates immiscibility of the polymers, the thermal analysis of the film showed also an increase in degree of crystallinity as the content of grafted nanowhiskers increased, this composition to 30/70. In the case of composites with composition 50/50 (PCL / PBSA) there was a decrease in the degree of crystallinity of polymers. The immiscibility of the polymers in the film was also confirmed by analysis DMTA where tanδ two distinct peaks were found for compositions 30/70, close to the glass transition temperatures of the two polymers. The same compositions processed via extrusion, and specimens injection molded, showed a decrease in thermal stability detected by TGA analysis. There was an increase in the degree of crystallinity of the PCL as the largest quantity of nanowhisker composites. The rigidity of the material was confirmed from the tensile test, where the elastic modulus increased approximately twice the percentage increase of nanofiller in the composites, as well as the decrease in percentage elongation and tensile strength has not changed much.
Language: Spanish
Subfield: Biomaterials
Open Access status: green
OpenAlex ID: W1814817703
Cites: 55
Cited by:
Related to: 8