Work

Avaliação da influência de diferentes tratamentos de superfície na resistência de união ao cisalhamento entre zircônia Y-TZP e o cimento resinoso

Year: 2012
Type: dissertation
Abstract: OBJECTIVES: first stage: validate shear test using a new device for standardized by comparing the values of bond strength (BS) with conventional shear test and microshear test, between zirconia and a resin cement with two surface treatments. Second stage: evaluate the effect of metal primers based on MDP by BS between YTZP and different types of resin cements. Third stage: evaluate Y-TZP surface treatments effect of two lasers (Nd:YAG and Er:YAG) and two sandblasting procedures, with Al2O3 (JAT) before final sintering and tribochemical slicatization after the final sintering, through the flexural resistance (FR) surface roughness (SR) and BS. Fourth stage: evaluate the bonding stability between zirconia and resin cement using a MDP-based primer or a high power laser, after thermal cycling. MATERIAL AND METHODS: BS Y-TZP specimens were prepared with dimensions of 6x6x3mm, and for FS test with 2,5x4,5x20 mm. In the first stage the surface treatments of the specimens were JAT+ Signum Ziconia Bond (SZB - Heraeus), tibochemical silicatization using Rocatec (ROC - 3MEspe) and control (CO - without treatment). In the second stage the primers used were Alloy-Primer (AP - Kuraray), SZB, Z-Prime Plus (ZP - Bisco), and the resin cements: Panavia F (Kuraray), NX3 (Kerr), set (SDI), Multilink (Ivoclair). During the third stage the tribochemical silicatization was perfomed using ROC. The shear bond strength device standardized was used to evaluate the BS of second, third and fourth stage. Test data for BS, SR were analyzed by ANOVA and Tukey test ( = 0.05) and FS by Kruskall-Wallis test ( = 0.05). RESULTS: first Stage: the microshear test groups behave as follow: JAT+SZB> ROC>CO, and for the other two shear tests following the ranking were obtained: JAT+SZB=ROC>CO. Second stage: the SZB showed higher BS for all cements when compared to control groups. The ZP values increased for Panavia F and NX3. AP values increased only for the seT cement. Third stage: BS values for JAT and Er:YAG were similar to ROC, and Nd:YAG was higher compared to the ROC. When evaluated by SR: Nd:YAG> Er:YAG>JAT> ROC, while for FS: ROC> JAT = Nd:YAG = Er:YAG. Fourth stage: after the shear test the following ranking was obtained: Nd:YAG 24h> Nd:YAG thermocycled = SZB 24h> SZB thermocycled. CONCLUSIONS: shear bond strength test with standardized device showed similar result to the conventional shear bond strength, and it can be considered a viable method for evaluating the BS. Treatment with Nd:YAG before the final sintering was effective in BS.
Language: Portuguese
Field: Dentistry
Open Access status: green
OpenAlex ID: W2111158076
Cites: 96
Cited by: 3
Related to: 8