Deformation Mechanisms of Toughened Poly(Lactic Acid) Using Novel Additives

Year: 2021
Type: dissertation
Abstract: Poly(lactic acid) (PLA) is a biopolymer that is certified biodegradable, but its inherent brittleness narrows the variety of useful commercial applications. The objective of this research is to promote the development of multi-functional additives that impart toughness and facilitate biodegradation of PLA. Novel additives were supplied by TRuCapSol, LLC for evaluation. Such particle-base additives are emulsion based but the active ingredients are proprietary. The goal of this work is to compare the toughening effectiveness of two types of multifunctional particles. NatureWorks, LLC. Ingeo� Biopolymer 4043D was chosen as most suitable PLA resin for blending with micron-size particles (MP) and submicron-size particles (SMP) provided by TRuCapSol, LLC. This PLA resin was thoroughly characterized using solution viscometry, FTIR analysis, melt rheology, TGA, and DSC. It was determined to have an Mv value of 122,000 g/mol, melt flow activation energy of 82 kJ/mol, and a thermal degradation temperature of 362?C. This PLA 4043D resin was melt compounded, via twin screw extrusion, with various amounts of MP or SMP. The extruded strands were pelletized, and the pellets were injection molded into tensile specimens. Particle dispersion, thermal stability, melt viscosity, tensile properties and mechanical deformation mechanisms were studied. Tensile, notched Izod impact, and thermal properties of injection molded specimens were also characterized. The resulting properties of both pellets and injection molded specimens were compared to two commercially available toughened PLA blends: PLAyPHAb and 3D870 grade (Pro PLA). Tensile and notched Izod impact fracture surfaces were characterized using SEM microscopy. All PLA 4043D blends containing novel multi-functional particles (PLA 4043D/MP or PLA 4043D/SMP) saw a decrease in zero-shear viscosity and melt flow activation energy when compared to neat PLA resin. However, zero-shear viscosity increased with increasing MP or SMP content, but overall remained lower than neat PLA resin. There was also a considerable decrease in zero-shear viscosity after injection molding due to high shear processing and/or another high temperature thermal excursion. Einstein�s equation failed to predict the melt viscosity of PLA 4043D/MP and PLA 4043D/SMP blends as a function of particle volume fraction as it did not account for plasticization or degradation effects by the particles on the matrix. There was negligible loss in thermal degradation temperature of PLA 4043D/MP and PLA 4043D/SMP blends when compared to neat PLA 4043D giving reassurance that processing temperatures did not affect the integrity of blends. The Tg of PLA blends were lower than neat PLA. Degree of crystallinity in the matrix was also decreased with MP or SMP content. Yield stress and stress at break of the blends decreased, but elongation at break increased with increasing MP or SMP content. PLA 4043D/10SMP saw the most drastic change in tensile properties when compared to neat PLA 4043D. A decrease in yield strength from 57 MPa to 36 MPa, stress at break from 53 MPa to 16.4 MPa, and an increase in elongation at break from 7% to 47% were observed. Yield strengths of PLAyPHAb and Pro PLA were the same as neat PLA 4043D resin. However, there elongations at break were slightly higher at 19.2% and 9.5%. Surprisingly and unexplainably the moduli of the PLA 4043D/MP and PLA 4043D/SMP blends did not decrease when compared to neat PLA resin and were maintained at 1.7 GPa. No necking occurred, but stress whitening along the length of the gage section of tensile specimens was enhanced by increasing particle content. MP and SMP facilitated massive crazing and matrix dilation of the PLA matrix. Notched Izod impact results showed no significant improvements to impact toughness. PLAyPHAb and Pro PLA blends had higher impact toughness values than neat PLA resin: 54 J/m, 56 J/m, and 44 J/m respectively. Crack propagation rate was too high for any significant plastic deformation to occur, and all specimens exhibited brittle fracture. SEM micrographs of PLA 4043D/MP and PLA 4043D/SMP blend tensile fracture surfaces reveal signs of good particle dispersion, ductile tearing at the inherent stress concentration that facilitated crack initiation. Less matrix deformation but more polymer fibril orientation was observed as the crack rate increased and propagated rapidly across the width of the tensile specimens. Exploration of the thermal and mechanical behavior of multi-functional particles blended with PLA provided valuable results for understanding the processability and potential product applications. The results from this project provided competitive results when compared to commercially available toughened PLA blends.
Institution: Lehigh University
Language: English
Subfield: Biomaterials
Open Access status: green
OpenAlex ID: W7132865233
Cites: 26
Cited by:
Related to: 10