Ternary solvation sheath reconfiguration drives sustainable cryogenic Li||Cl2 batteries

Year: 2026
Type: article
Abstract: Rechargeable Li | |Cl2 batteries hold promise for low temperature storage but suffer from interfacial instability due to electrolyte decomposition, particularly at cryogenic temperatures. We identify the failure mechanism as a complex solvation chemistry involving Li+, reactive SOCl2, and coordinating chloroaluminates that drives parasitic reactions. Here, we demonstrate a Ternary Solvation Sheath Reconfiguration strategy using lithium trifluoromethanesulfonate to engineer the solvation structure. By leveraging strong anion-cation interactions, this approach reconfigures the coordination environment to displace solvent molecules and directs the in-situ formation of a robust, bilayered positive electrode electrolyte interphase featuring an inorganic-rich inner layer. This engineered interphase effectively suppresses electrolyte degradation and enhances charge-transfer kinetics by lowering the Li+ desolvation barrier. Consequently, cells employing the Ternary Solvation Sheath Reconfiguration electrolyte sustain stable cycling at –40 °C (1000 mA g⁻1), maintaining capacity retention of 99.2% and Coulombic efficiency of 99.2% after 1100 cycles, while enabling reliable operation even at –80 °C. This work establishes a systematic framework for designing functional interphases via solvation chemistry for sustainable energy storage. Cryogenic Li | |Cl2 batteries face severe interfacial instability. Here, authors demonstrate a solvation reconfiguration strategy to build a robust interphase, enabling stable cycling of Li | |Cl2 batteries for over 1100 cycles at –40 °C.
Language: English
Open Access status: gold
Estimated APC paid: $6,990
OpenAlex ID: W7133833488
FWCI: 3.411
Cites: 32
Cited by: 2
Related to: