Year: 2022
Type: dissertation
Abstract: Alkali-activated materials (AAMs), including those classified as geopolymer, have been studied in the past year.These materials have demonstrated desirable mechanical strengths and high fire resistance properties, making them an ideal substitute for Portland cement in a wide range of applications.However, the extensive application of AAMs in construction fields is limited by several factors.This thesis reports the characterizations of geopolymers and alkali-activated slag and their durability, including fire resistance, alkali leaching, and efflorescence formation.Five series of geopolymer were prepared with various dosages (0%, 15%, 30%, 45%, and 60%) of ground granulated blast-furnace slag (GGBS) used to replace fly ash.The incorporation of GGBS was found to significantly increase the compressive strength due to the formation of a denser microstructure compared to the matrix containing no GGBS.However, after exposure to elevated temperature, the geopolymer containing a high amount of Ca from GGBS behaved differently from that of low-Ca geopolymer.Low-Ca geopolymer exhibited microstructure densification, while high-Ca geopolymer presents a highly porous microstructure caused by the C-S-H gel decomposition after exposure to a temperature above 500 ℃.Despite exhibiting a highly porous microstructure, the specimens could maintain enough strength when using GGBS up to 45%.When replacing fly ash with 60% GGBS, the specimen suffers from spalling and significant strength loss.Using KOH solution could improve the strength of fly ash/geopolymer by sintering that occurs at a temperature lower than the sintering temperature of geopolymer produced using NaOH solution.Efflorescence, the white deposits on the surface of the material, is one of the major issues limiting the application of alkali-activated materials.Efflorescence in AAMs is strongly related to the alkali particles that remain unreacted in the matrix.Despite a very compact structure, a rapid efflorescence formation was observed in alkali-activated slag.This finding proves that low-porosity material does not necessarily mean a low tendency to efflorescence.Incorporating a small amount of silica fume up to 15% was found to reduce the efflorescence formation.This indicates that modifying the chemical composition can help control the efflorescence formation in alkali-activated slag.The extensive application of AAMs is also limited by their brittle behavior.To overcome this issue, epoxy resin was added into a geopolymer mixture.The binder consists of 55% fly ash and 45% slag, while small amounts of epoxy resin (1% and 2.5% of the binder mass) were incorporated to produce geopolymer composite.The results show that the inclusion of epoxy resin significantly enhances the mechanical properties and reduces the total alkali leaching of ambient-cured geopolymer, thus promising the application in construction industry.Interestingly, despite significant loss of alkali, specimens immersed in water present a higher compressive strength than that of cured at ambient temperature.
Author: Saludung, Apriany
Institution: Hiroshima University
Language: English
Subfield: Civil and Structural Engineering
Field: Engineering
Domain: Physical Sciences
Keywords: geopolymer, alkali-activated slag, ground granulated blast furnace slag, fly ash replacement, fire resistance, compressive strength, microstructure densification, alkaline leaching, efflorescence, silica fume, epoxy resin, brittleness, alkali-activated materials, cement replacement, spalling
Open Access status: green
OpenAlex ID: W7144756973