アルカリ金属塩化物添加のもとでNb 2 O 5 と非晶質ホウ素によるNbB 2 の合成および磁化率
Year: 2017
Type: article
Abstract: NbB_2(hexagonal)powders were prepared by the solid-state reaction between niobium(V^{5+}) oxide Nb_2O_5, and amorphous boron powders with 5 mass% AECl(AE=Li, Na, K)at reaction temperatures of 873 to 1473 K for 2 h in an argon atmosphere. When the mole ratio B/Nb_2O_5 in the starting materials was 9.0, the single phase of NbB_2 was obtained at reaction temperature of 1023 K, 600 K lower than without the additives. When the AECl was not added, the single phase of NbB_2 formed at up to 1573 K exhibited particles with a grain size of approximately 10μm in diameter. When AECl was added, the product formed at soaking temperature of 1023 K exhibited particles with a grain size of approximately 0.1μm in diameter. The lattice parameters of NbB_2 changed a=0.3111~0.3084 nm and c=0.3264~0.3308 nm. This study processes are available for the production of NbB_2 such as the thermal reduction of the Nb_2O_5 with boron for addition AECl. Magnetic susceptibility of powder samples of NbB_2 was measured by using a SQUID magnetometer in the temperature range of 300 K to 1.8 K.
Source: 国士舘大学理工学部紀要
Language: Japanese
Subfield: Ceramics and Composites
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W3147730919