Work

Use of Glow Discharge Plasma for Deposition Wear Resistant Cvd Diamond Coatings to Cutting Tools With Pcd

Year: 2026
Type: article
Abstract: To improve the wear resistance of cutting tools equipped with inserts sintered from synthetic diamond powder, processes have been developed for synthesizing polycrystalline diamond coatings on their surface using the CVD method from H2/CH4 gas mixture in a glow discharge stabilized by a transverse magnetic field. Homogeneous coatings with a thickness of 17…56 μm and a clearly formed microcrystalline structure were obtained. A comparison was made between the DC and pulsed modes of operation of the discharge power source during the preparatory treatment of the cutting inserts surface and directly during the deposition of the coating. The advantages of the pulsed mode (frequency 50 kHz, duty cycle 1.1) at the preparatory treatment stage were revealed, which ensures rapid cleaning and heating of the cutting inserts surface to a synthesis temperature of 1070…1150 °C without the glow discharge transitioning to an arc discharge. It has been found that the deposition rate and surface morphology of coatings synthesized in pulsed and DC modes do not differ significantly. As the coating thickness increases, the average size of diamond crystals increases. It has been shown that the deposition of diamond coating increases the wear resistance of cutting tools when machining difficult-to-machine materials (ceramics, hard alloy) by more than 1.5 times. A coating with a thickness of 56 μm, deposited by DC mode, provided the tool with the greatest wear resistance when turning the VK8 hard alloy, however, the increase in diamond crystal size led to a deterioration in the quality of the machined surface due to an increase in its roughness. The feasibility of optimizing the size of diamond grains to improve the performance characteristics of the tool is discussed.
Language: English
Open Access status: bronze
OpenAlex ID: W7155504624
FWCI:
Cites: 16
Cited by:
Related to: 10