Contouring mitigates voiding at the lithium/ceramic electrolyte interface on discharging solid-state batteries
Year: 2026
Type: article
Abstract: Interfacial void formation during discharge limits the practical performance of lithium metal solid-state batteries. Here we show that introducing an egg-box topography at the Li/Li 6 PS 5 Cl interface increases the discharge current at which voiding commences tenfold, from 0.2 to 2 mA cm −2 at 2 MPa and 30 °C. The contoured interface also sustains pulsed currents up to 3 mA cm −2 at 30 °C and 8 mA cm −2 at 60 °C without cell failure. Under these conditions, it does not completely eliminate void formation but suppresses void growth and associated voltage polarization. Consequently, it sustains discharge profiles derived from the Worldwide Harmonized Light Vehicles Test Procedure, representing realistic electric vehicle driving demands, whereas non-contoured interfaces fail rapidly. A full cell with a thin contoured solid electrolyte retains this advantage over its non-contoured counterpart. Contouring the Li/solid electrolyte interface is therefore an effective strategy for enabling practically relevant discharge rates in solid-state batteries.
Source: Nature Energy
Language: English
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: hybrid
Estimated APC paid: $12,690
OpenAlex ID: W7163538630