Abstract: SiC-based ceramic matrix composites (CMCs), such as carbon fibres reinforced silicon carbide (C/SiC) or silicon carbide fibres reinforced silicon carbide (SiC/SiC), are prime candidates for the components for aerospace and nuclear applications performing at extreme conditions. A critical issue for the wider utilisation of these materials is the development of inexpensive and reliable joining methods to assemble large components into complex structures. In this work, Spark Plasma Sintering (SPS) and Flash-SPS were employed to join monolithic CVD-SiC and CMCs via indirect and direct heating of the joined component, respectively. A temperature as low as 1300 degrees C was sufficient to achieve a defect-free joining interface when a MAX phase, Ti3SiC2, was applied as the joining interlayer. The joints retained 70% of their initial room temperature strength at 1200 degrees C. Conformal behaviour of the Ti3SiC2 foil and its infiltration into the surface cracks in the CVD-SiC coating of CMCs resulted in the apparent shear strength of the CMCs up to ~32 MPa. When a Ti foil was used as the interlayer, the temperature of 1700 degrees C had to be used to obtain sound joints. For the same joints, however, a significant reduction of both the joining temperature (to ~1250 degrees C) and the process time (to 8 s) was observed when a direct Flash-SPS joining process of CMCs with the Ti foil was employed (the maximum heating power of 2.2 kW). The apparent shear strength of the joints matched the interlaminar shear strength of the composites. A sound joint was obtained by forming a metallic kind of joint (Ti-based) at the joining temperature, in which the absence of any reaction phases (titanium silicides, carbides or ternary phases) significantly shortened the time necessary for the solid-state diffusion bonding. Such a reduction in processing time and temperature leads to energy savings and potentially higher industrial interest in the process. In order to decrease a thermal mismatch between SiC-based matrix and joining materials, a so-called seamless joining approach was also applied. This consists of the utilization of rare-earth (RE) based ternary layered materials (RE3Si2C2) as the joining filler, followed by their decomposition during joining, which left behind near-seamless joints.
Language: English
Open Access status: green
OpenAlex ID: W7202012017
Cites:
Cited by:
Related to: 10