EDM fine dressing formed diamond grinding wheel test
Year: 2026
Type: article
Abstract: ObjectivesIn today's information age, the semiconductor industry, as one of the core fields of modern science and technology, is booming at an astonishing speed. However, in the process of rapid development, a problem that can not be ignored has gradually emerged. That is, the processing technology and equipment of key wafer chamfering grinding wheels have been monopolized by foreign countries for a long time. This not only poses a major challenge to the independent development of Chinese semiconductor industry, but also limits the diversified development of the global semiconductor industry to a certain extent. The multi-micro-groove diamond grinding wheel has become the best choice for achieving high-quality wafer chamfering due to its excellent performance, which has high hardness, high wear resistance and high precision characteristics, and can achieve efficient and precise processing during wafer chamfering to ensure wafer quality and performance. However, the processing technology of multi-micro-groove forming diamond grinding wheel has always been a difficult problem in the industry, involving the complex material technology, the processing technology, the precision measurement technology and many other fields. To this end, the electrical discharge machining (EDM) finishing platform is set up, and the EDM finishing method is used to process the high-precision multi-micro-groove forming diamantine wafer chamfering wheel, and the finished wheel meeting the requirements is obtained.MethodsBy using the EDM dressing method, the influences of dressing factors such as voltage, discharge current and pulse width on the discharge rule are explored one by one. The orthogonal tests are carried out on their effects on the shape, contour accuracy and surface machining quality of the grinding wheel, and the combination of process electrical parameters for grinding wheel finishing is obtained and verified.ResultsThe optimized process parameter combination for grinding wheel dressing is the voltage of 50 V, the discharge current of 3 A and the pulse width of 40 μs. Under this combination of parameters, the surface of the grinding wheel finally obtains a qualified groove type with the groove depth of 596.35 μm, the circular arc radius of 178.72 μm and the groove angle of 44.25°. The smoothness of both sides of the groove is good, the edges are neat and clear, the scratches are fine and uniform, and there are no obvious burrs or edge breaks on the surface. Additionally, there are no cracks or thermal deformations on the grinding wheel surface.ConclusionsThis study provides theoretical basis and process test reference for EDM dressing of chamfered grinding wheel, and promotes higher quality and wider application of this method in the field of grinding wheel dressing. In addition, through the performance test of the graphite wafer chamfering grinding wheels after dressing, it is found that the high precision formed grinding wheel obtained by dressing has good practical value and application prospect.
Authors: FANG Zhou, MEI Lifang, CHEN Genyu, LU Enhao
Language: Chinese
Subfield: Industrial and Manufacturing Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W7203564628