Abstract: Objective Massive fresh water and river sand consumption in traditional concrete manufacturing brings severe resource depletion and ecological environmental damage, which restricts the sustainable development of marine infrastructure construction. As a feasible alternative building material, seawater sea-sand concrete (SSC) directly utilizes seawater and un-desalted sea sand as raw materials, effectively reducing the reliance on limited terrestrial freshwater and river sand resources. Nevertheless, inherent defects including high brittleness, low tensile strength and rapid crack propagation seriously restrict the large-scale popularization and engineering application of plain SSC. Fiber reinforcement technology has been widely verified as an effective modification approach to optimize the tensile mechanical performance and anti-fracture capacity of cement-based composites. Polyvinyl alcohol (PVA) fiber possesses outstanding hydrophilicity, high tensile modulus and excellent interfacial bonding performance with cement matrix, which exhibits great potential to improve the crack resistance of SSC. Existing relevant researches mostly concentrate on the compressive strength and flexural performance of PVA fiber reinforced SSC, while systematic investigations on splitting tensile mechanical behaviors and real-time internal damage evolution laws remain insufficient. The present work targets the splitting tensile performance and multi-stage damage evolution characteristics of PVA fiber reinforced SSC under uniaxial splitting load, and the quantitative correlation between fiber volume fraction, tensile mechanical indexes and acoustic emission (AE) damage parameters is revealed. The obtained test data and damage regulation mechanism can supply theoretical basis and technical reference for material proportion design, crack control and safe service evaluation of SSC applied in marine engineering structures.MethodsSSC matrix mixed with natural sea sand and artificial seawater was prepared as the base material, and PVA fiber with fixed length was incorporated into concrete matrix with gradient volume fractions of 0%, 0.5%, 1.0%, 1.5%, 2.0% and 2.5%. Standard cylindrical specimens with unified size were cast, cured under standard marine environment simulation conditions to reach complete design strength before mechanical tests. Brazilian splitting test scheme was adopted to characterize the splitting tensile mechanical properties of SSC specimens with different fiber dosages. Meanwhile, high-precision AE real-time monitoring system was arranged on the surface of test specimens to capture continuous AE signal waveforms during the whole splitting loading process. Key AE characteristic parameters including b-value, dominant frequency distribution, signal proportion of different frequency bands and crack type classification ratio were extracted and calculated after test completion. The influence mechanism of PVA fiber volume fraction on splitting tensile strength, post-peak ductility, failure mode and multi-stage damage evolution of SSC was quantitatively analyzed through comparative analysis between plain reference group and fiber modified groups.Results and Discussions The splitting tensile bearing capacity and post-crack deformation ductility of SSC are significantly promoted with the addition of PVA fibers. The splitting tensile strength presents an obvious variation trend of first rising and then falling with the increase of fiber volume fraction. The peak splitting tensile strength of 3.27 MPa is achieved at the fiber volume fraction of 1.5%, which represents the optimal fiber dosage for tensile performance improvement. When fiber dosage is lower than 1.5%, dispersed PVA fibers distributed inside the matrix form uniform fiber network structures. The fiber bridging effect and crack arresting effect take full effect under tensile load, which restrain the rapid expansion of primary cracks and delay the occurrence of instantaneous brittle failure. Excess fiber addition exceeding 1.5% leads to uneven fiber dispersion and local fiber agglomeration inside concrete matrix, which introduces extra internal initial defects and weak interfacial zones, resulting in the gradual decline of splitting tensile strength. PVA fibers induce the generation and coordinated expansion of a large number of tiny microcracks inside specimens, and the macroscopic failure mode is transformed from sudden brittle splitting failure controlled by a single penetrating main crack to progressive ductile failure with multi-crack synchronous propagation. The whole splitting damage evolution process of SSC is divided into four typical stages according to the variation rule of AE signal activity, including initial microcrack compaction stage, stable microcrack growth stage, unstable crack expansion stage and post-peak residual bearing stage. The b-value of AE signals gradually decreases with continuous loading, and the b-value drops to the range of 0–0.5 when external load reaches peak splitting tensile load, which acts as an early warning index for critical failure of SSC. The dominant frequency of all AE signals generated in splitting tests distributes within the range of 0–500 kHz. In the unstable crack propagation stage, the proportion of high-frequency AE signals of PVA fiber modified specimens ranges from 4.86% to 6.76%, which is 42.1%–97.7% higher than that of plain reference specimens labeled JZ-0. Compared with the reference group, the dominant frequency band of fiber-reinforced specimens migrates to high-frequency region earlier and changes more gently during loading. The proportion of pre-peak high-frequency signals of modified specimens is remarkably higher than that of plain SSC, while the proportion of post-peak high-frequency signals decreases monotonously as fiber volume fraction increases. Tensile cracks constitute the dominant damage form throughout the splitting loading procedure, and the proportion of shear cracks rises continuously with the aggravation of internal damage. In the critical unstable crack propagation stage, the tensile crack proportion of plain reference specimens reaches 91.2%. The incorporation of PVA fibers effectively reduces the tensile crack ratio to 82.3%–90.2%, which alleviates the severe brittle tensile failure tendency of SSC matrix and enhances the overall damage tolerance of concrete materials..Conclusions The regulation law of PVA fiber volume fraction on splitting tensile mechanical performance and multi-stage internal damage evolution of SSC is clarified through combined splitting mechanical tests and AE real-time monitoring. Proper incorporation of PVA fibers optimizes tensile bearing capacity, improves post-peak ductility and transforms the brittle failure mode of SSC. The variation characteristics of AE b-value, dominant frequency distribution and crack classification ratio can quantitatively reflect the internal damage degree and failure precursor information of fiber reinforced SSC under splitting load. The established quantitative correlation between fiber dosage, tensile mechanical indexes and AE damage characteristic parameters provides clear experimental support for the crack resistance design and damage monitoring of SSC structures serving in marine corrosive environments. The research results offer reliable technical guidance for the popularization and safe application of seawater sea-sand concrete in coastal breakwaters, marine docks and other marine infrastructure projects.
Language: Chinese
Open Access status: diamond
OpenAlex ID: W7204152782
FWCI:
Cites:
Cited by:
Related to: 10