Effect of Zirconia Surface Treatments on the Bond Strength of Composite Resin in Ceramic Repair
Year: 2026
Type: conference-paper
Abstract: The chipping of veneering ceramics from a zirconia core is a common cause of prosthetic rehabilitation failure, which is why various composite restoration protocols have been developed to establish morphological and functional integrity of the restoration. To examine the bond strength between zirconia and composite resin used for repair applying different zirconia surface preparation protocols. Plate-shaped specimens (1×5×10 mm) were fabricated from monolithic zirconia (Honchon Smile, Changsha Honchon Technology Co., Ltd., China) using the CAD/CAM method and divided into three groups according to the surface preparation protocol. The first group of specimens was sandblasted with Al₂O₃ particles (50 µm; 1–2 bar; 10 mm; 45°), followed by cleaning with isopropanol and application of MDP primer (Z- Prime Plus). The second group was mechanically treated with a diamond bur, followed by the application of a universal primer containing MDP (Monobond Plus). The third group was treated by tribochemical silcatization (SiO₂), and the application of a universal primer containing MDP (Monobond Plus). A composite resin for repair (Tetric EvoCeram, Ivoclar Vivadent) was applied to all samples using a layered technique. The bond strength was tested on a universal testing machine (Shimadzu AGS-X) at a speed of 1 mm/min until fracture occurred at the interface of zirconia and composite. The first group showed significantly higher values of fracture force (332.47 ± 172.81 N) and bond strength (8.31 ± 4.32 MPa) compared to the second group (153.79 ± 77.74 N; 3.84 ± 1.94 MPa), (p<0.01). The third group also showed higher values (310.00 ± 150.00 N; 7.89 ± 4.85 MPa) compared to the second (p<0.01), but without significant difference compared to the first group (p>0.05). The samples of the first and third groups showed higher deformation, absorbed energy and displacement at failure compared to the second group, which indicates higher joint resistance. Treatment with Al₂O₃ particles and tribochemical silcatization showed higher fracture resistance, with higher material durability (absorbed energy, displacement and percent of deformation), indicating the importance of micromechanical retention and chemical adhesion.
Language: English
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: green
OpenAlex ID: W7204348021
