Work

Investigation of the initial stage of iron oxidation in the air. Part 2. Temperature range 400-625 ºС

Year: 2019
Type: article
Abstract: Iron oxidation in the case of formation of thin oxide films on the surface of iron plates as a result of their oxidation in air by a parabolic law at temperatures above(400-550 ºС) and below (575 – 600 ºС) the Shadronpoint (575 ºС)has been studied.Studies are performed on the experimental plant described in the first part of the article, published in this issue of the journal.The experimental determination of the thickness of the oxide film depending on time is based on the method of occurrence of "variability" colors on the surface of the oxidized iron plate. With an increase in the thickness of the oxide film its color as a result of light's interference will consistently vary according to the series: yellow, orange, red, purple, violet and blue. This corresponds to the range of the oxide film's thickness from 46 to 72 nm.In the temperature range of 400-550 °C, a stable oxide Fe3O4 (magnetite) appears on the iron’s surface. It was shown that the dependences lnh of lnτ for all investigated temperatures are linear and have tangents of inclination angles equal to 0.5. The obtainedvalue of the activation energyis constant and equal to E = 43.0 kJ/mol.The oxygen diffusion coefficient D = 1.73 · 10–13 m2/s was obtained according to the oxidation model of a metal plate, which is based on the determinant role of oxygen diffusion through an oxide film.In the temperature range of 550 - 625 ºC, the change in the rate of the constant of the interaction between iron and oxygen from the air is due to the stable formation ofawustiteFeO. All of the oxidation isotherms can be described by the linear dependence in the coordinates lnh and lnτ. It was shown that the index of degree in the oxidation law at the temperatures below the Shadronpoint is equal to 2 (the parabolic law), and above the Shadron point it increases with increasing temperature of the process in accordance with the obtained dependence n = 2 + 0.008 (T-823).
Language: English
Open Access status: diamond
OpenAlex ID: W2954684057
FWCI:
Cites:
Cited by:
Related to: 10