Spin-Coating-Speed-Dependent Structural and Optical Properties of Open-Air-Processed MAPbI 3 Thin Films with Bandgap-Constrained SCAPS-1D Sensitivity Analysis
Year: 2026
Type: preprint
Abstract: Spin coating offers an accessible route for depositing metal-halide perovskite absorbers, but interactions among rotational speed, solvent removal and crystallization complicate ambient process optimization. This study examined the effects of spin-coating speed (2000–5000 rpm) on the structural and optical properties of open-air-processed methylammonium lead iodide (MAPbI₃) films and used measured optical bandgaps to constrain SCAPS-1D simulations. Films were deposited from a 1.25 M precursor using ethyl acetate antisolvent treatment and annealed at 110°C for 10 min under controlled conditions of 24.4°C and 41.5% relative humidity. X-ray diffraction confirmed tetragonal MAPbI₃ with preferential (110) orientation and no detectable PbI₂ reflection. The structural response was non-monotonic. At 3000 rpm, the film exhibited the narrowest (110) peak (FWHM: 0.352°), largest Scherrer coherent-domain size (22.73 nm), lowest estimated microstrain (1.257 × 10⁻²) and lowest crystallographic dislocation-density parameter (1.936 × 10⁻³ nm⁻²). Thus, 3000 rpm produced the most favourable XRD-derived crystalline characteristics within the investigated range, although these metrics do not establish reduced electronic trap density, suppressed recombination or superior photovoltaic performance. Optical bandgaps ranged from 1.59–1.60 eV. In an otherwise fixed FTO/TiO₂/MAPbI₃/Spiro-OMeTAD/carbon model, the corresponding simulated efficiencies were 16.67% and 16.47%, respectively. Coordinated parameter optimization yielded a projected efficiency of 25.38%, with \(\:{V}_{oc}\) of 1.25 V, \(\:{J}_{sc}\) of 24.24 mA cm⁻² and fill factor of 83.61%. These results establish a process-specific structure–optical-property relationship, while the simulated outputs remain model-dependent projections requiring experimental device validation. The approach also illustrates how experimental measurements can inform device-level sensitivity analysis without overstating causal relationships.
Source: Research Square
Language: English
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
Funder: UK Research and Innovation
OpenAlex ID: W7225984768