Fluoride release and surface properties of conventional and resin-modified glass ionomer cements following distilled-water storage and simulated gastric-acid exposure
Year: 2026
Type: article
Abstract: Glass ionomer cements (GICs) are extensively used in restorative dentistry because of their chemical adhesion to tooth structure and sustained fluoride release. Their physicochemical and optical properties may be influenced by the environmental conditions to which they are exposed. This in vitro study compared fluoride release, surface microhardness, gloss, and color change of a conventional GIC and a resin-modified GIC (RMGIC) following either prolonged distilled-water storage or an accelerated simulated gastric-acid exposure protocol. A total of 32 disk-shaped specimens were prepared for each of two materials: a conventional GIC (Ketac Molar Easymix) and an RMGIC (Fuji II LC). For each material, 16 specimens were allocated to Vickers microhardness testing and 16 to surface-related measurements. For each outcome assessment, 8 specimens were assigned to distilled-water storage at 37 °C for three months and 8 to exposure to simulated gastric juice (pH 1.2) at 37 °C for 2 h 15 min. The shorter gastric-acid exposure was selected based on a previously reported exposure-equivalence model, according to which 45 min of continuous exposure approximates one month of cumulative clinical gastric-acid contact. Thus, the two protocols were intended to represent approximately three months of their respective environmental exposures, although the actual exposure durations differed substantially. Fluoride release was quantified using a spectrophotometric method. Surface microhardness was evaluated with the Vickers microhardness test, gloss was measured using a glossmeter, and color stability was assessed according to the CIEDE2000 (ΔE₀₀) color difference system. Statistical analyses were performed using appropriate parametric or non-parametric tests with a significance level of 5%. The two exposure protocols yielded different material-specific outcomes. Ketac Molar Easymix showed higher fluoride release under the simulated gastric-acid protocol than under distilled-water storage (3.81 ± 0.1 vs. 3.38 ± 0.4 mg/L; p = 0.013), whereas Fuji II LC showed lower fluoride release (2.96 ± 0.3 vs. 3.87 ± 0.2 mg/L; p < 0.001). Fuji II LC exhibited lower microhardness under the simulated gastric-acid protocol than after distilled-water storage (10.2 ± 5.1 vs. 24.3 ± 4.9 VHN; p < 0.001), whereas no significant difference was observed for Ketac Molar Easymix (68.6 ± 7.7 vs. 70.3 ± 7.5 VHN; p = 0.658). Fuji II LC exhibited higher gloss (42.5 ± 5.9 vs. 2.2 ± 0.2 GU) and lower color change (ΔE₀₀: 1.9 ± 1.3 vs. 10.2 ± 5.4) than Ketac Molar Easymix under the simulated gastric-acid protocol (both p ≤ 0.001). Within the limitations of this in vitro study, the tested conventional and resin-modified GICs exhibited distinct fluoride-release and surface-property profiles under the two experimental exposure protocols. The findings suggest that material composition and environmental exposure conditions may jointly influence the physicochemical and optical behavior of glass ionomer-based materials. However, because the exposure medium and duration differed between the experimental protocols, the observed differences cannot be attributed exclusively to the effect of gastric acid. These findings underscore the importance of considering material-specific physicochemical characteristics when selecting restorative materials for patients experiencing recurrent gastric acid exposure.
Source: BMC Oral Health
Institutions: Trakya University, Beykent University
Language: English
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: gold
Estimated APC paid: $3,190
OpenAlex ID: W7226009943