Abstract: This study evaluated the effects of polishing systems, staining media, and aging on the optical properties of permanent 3D-printed restorative materials compared with a computer-aided design/computer-aided manufacturing (CAD/CAM) material. Three permanent 3D-printed restorative materials (VarseoSmile Crown Plus, Saremco Print Crowntec, and Formlabs Permanent Crown) and one CAD/CAM material (Grandio Blok) were evaluated. Specimens were polished using four polishing systems (PS) or left unpolished and immersed in distilled water, coffee, or red wine for 24 h, 7 days, and 30 days. Color change (ΔE₀₀), translucency parameter (TP), and contrast ratio (CR) were measured using a spectrophotometer. Data were analyzed statistically (α = 0.05). Color change increased significantly over time in all groups ( p < 0.05). Red wine produced the highest ΔE₀₀ values, whereas distilled water caused the lowest discoloration. Polished specimens generally exhibited lower discoloration than unpolished controls. TP decreased over time, particularly after coffee and red wine immersion, whereas CR increased. The CAD/CAM material demonstrated greater optical stability and translucency preservation than the 3D-printed materials. Material type, polishing protocol, staining medium, and aging significantly influenced optical properties. Surface polishing improved color stability and translucency preservation, whereas coffee and red wine adversely affected the long-term optical performance of both CAD/CAM and 3D-printed restorative materials.
Source: BMC Oral Health
Institution: Akdeniz University
Language: English
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: gold
Estimated APC paid: $3,190
OpenAlex ID: W7232107784