Abstract: This study examines how castor oil (CST), palm olein (PLM) and dioctyl adipate (DOA) affect the cure kinetics, processing window and network properties of a highly filled (79.87 wt% solids) AP/Al/HTPB/TDI propellant (NCO/OH = 0.94) relative to an unplasticized (UNP) baseline. Cure (ATR-FTIR) and slurry viscosity were followed at 50, 60 and 70 °C for two independent batches per system. Seven kinetic models were ranked by AICc and screened for parameter identifiability by residual bootstrap. The Kamal–Sourour autocatalytic constant was not identifiable; all parameters of a two-step second-order model were. The C = C band at 1620–1660 cm⁻¹, a common internal reference for HTPB, grew about 1.5-fold during cure relative to two independent bands, so results were checked with all three. Castor oil was the only plasticizer that accelerated the cure with every reference (k₁(60 °C) 16.1–17.7 versus 9.1–10.0 × 10⁻³ min⁻¹; t₅₀ 57–62 versus 100–110 min), consistent with its hydroxyl groups acting as co-curative. DOA and PLM cured no faster than UNP, and the late-stage cure of DOA slowed. All plasticizers lengthened the time to the 10⁴ P casting limit at 50 °C (UNP 68 min; CST 119, DOA 127, PLM 138 min), PLM giving the widest and least temperature-sensitive window. Diffusion control at high conversion remained unresolved. With network data for the same formulations (crosslink density 40–54% of UNP), the results show that cure rate, processing window and network structure respond differently to the plasticizer and must be characterized separately.
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: diamond
Funder: Badan Riset dan Inovasi Nasional
OpenAlex ID: W7232156252