On the stored energy of severely deformed commercially pure titanium: A differential scanning calorimetry study
Year: 2026
Type: article
Abstract: Commercially pure titanium (CP-Ti) was subjected to multi-directional forging (MDF) with intermediate annealing for thermal analysis through differential scanning calorimetry (DSC). MDF processing increased the microhardness of CP-Ti up to 261 HV with 51% increment from the as-received material through strain hardening. Annealing the material after one MDF cycle at 450 °C and 650 °C relieved the internal stress and reduced the microhardness from 257 HV by ~8% and 35%, respectively. Strain hardening resulted in a decrease of thermal stability by up to 45% in the deformed samples, compared to 568 °C for the as-received sample. Analysis of stored energy using DSC indicated that recrystallization-related processes were the main contributors. Recrystallization temperature decreased from 688 °C to 581 °C, accelerating the recrystallization process as MDF cycles continued. The stored energy increased significantly from 0.92 J/g to ~5 J/g with subsequent MDF processing. The reason for these observations is ascribed to the increase in driving force for the recrystallization of MDFed samples, leading to lower recrystallization activation energy. The stored energy obtained from the DSC measurements was found to correlate well for the first cycle of MDF processing with stored energy estimates derived from the microhardness data through a dislocation model, with only ~10% deviation. The deviations between two stored energy evaluation methods increased notably with each intermediately annealed MDF cycle.
Source: Next Materials
Authors: Mohammad Zare, Mohammad Ali Mostafaei
Institution: Shahid Beheshti University
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: gold
Estimated APC paid: $1,280