Effect of CO2 laser treatment on adhesive properties of basalt fiber reinforced plastics adhesive joints
Year: 2026
Type: article
Abstract: In recent years, the adhesive bonding of fiber reinforced plastics (FRP) has been gaining attention as a method for achieving weight reduction in automobiles. Previous studies have focused on exposing fibers through laser treatment with the aim of improving adhesive strength. However, the effects of exposed fiber orientation and exposed fiber area on adhesive strength have not been clarified. The purpose of this study is to investigate the effect of fiber exposure conditions altered by the irradiation direction of CO2 laser treatment applied to the surface of basalt fiber reinforced plastics (BFRP) on the adhesive strength of BFRP. Plain woven basalt fabrics were used as the reinforcement material to vary the direction and area of exposed fibers formed as a function of the CO2 laser irradiation direction. The results of single lap shear tests indicated that exposing fibers parallel to the loading direction improved the adhesive strength. The 90° pattern exhibited a 23 % higher adhesive strength than the 0° pattern. However, increasing the exposed fiber area did not lead to an improvement in adhesive strength. Therefore, it was found that changing the fiber exposure direction provides a reinforcing effect within the adhesive layer, whereas the effect of the exposed fiber area on the adhesive strength characteristics of BFRP was found to be small.
Source: Journal of Textile Engineering
DOI: 10.4188/jte.260331a
Authors: Masaki ARAI, Yuto HAMADA, Takao OTA
Language: English
Subfield: Mechanical Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W7234187733