Enhanced conductivity and chemical durability of SPEEK membranes by cerium-silica incorporation for low-humidity PEM fuel cells
Year: 2026
Type: article
Abstract: This study addresses the conductivity durability trade-off that limits sulfonated poly(ether ether ketone) (SPEEK) membranes under low-humidity proton exchange membrane fuel cell (PEMFC) operation by incorporating a single sol–gel-derived Ce:SiO 2 hybrid nanofiller that combines hygroscopic water retention with radical-scavenging functionality. Raman spectroscopy confirmed the formation of a CeO 2 /SiO 2 composite in which crystalline cubic CeO2 (F 2 g mode at 465 cm⁻¹, with defect-related bands near 525 and 608 cm⁻¹) coexists with an amorphous silica phase, and together with FTIR provided evidence of interfacial Si–O–Ce bonding. SPEEK–Ce:SiO 2 composite membranes with 1, 5, and 10 wt% filler loadings were prepared by solution casting. Scanning electron microscopy confirmed filler incorporation but revealed partial agglomeration that became pronounced at 10 wt%, while AFM showed that filler addition markedly increased surface roughness and produced hill-like protrusions corresponding to the nanofiller and its agglomerates, consistent with the mechanical and conductivity trends. The SPEEK-Ce:SiO 2 (5%) composite gave the best balance of properties: proton conductivity reached 3.7 × 10⁻² S/cm at 30 °C, compared with 4.07 × 10⁻³ S/cm for bare SPEEK, and tensile strength increased from 1185.44 to 3144.07 kPa. Oxidative stability testing at 80 °C with 3 ppm Fe²⁺ showed the highest residual weight (81.6%) for the 5 wt% membrane after 250 min. In single-cell tests at 60 °C and 40% relative humidity, this membrane delivered a maximum power density of 50 mW/cm² at 130.2 mA/cm², versus 35 mW/cm² for bare SPEEK, and exhibited an open-circuit-voltage decay rate of only 0.04 mV/h compared with 0.35 mV/h for the pristine membrane. These results show that a 5 wt% Ce:SiO 2 loading simultaneously improves conductivity, oxidative stability, and low-humidity fuel-cell durability, indicating that the hybrid filler is a promising route to more robust SPEEK-based PEMs.
Source: Next Nanotechnology
Authors: Mayetu Segale(Conceptualization, Investigation, Software, Writing – original draft, Writing – review & editing), Dieketseng Tsotetsi(Formal analysis, Writing – review & editing), Tumelo Seadira(Writing – review & editing), Olayemi J. Fakayode(Formal analysis, Software, Visualization, Writing – review & editing), Tau S. Ntelane(Formal analysis, Writing – review & editing), Mokhotjwa Dhlamini(Writing – review & editing), Touhami Mokrani(Writing – review & editing), Bakang Mothudi(Writing – review & editing), Rudzani Sigwadi(Supervision)
Institution: University of South Africa
Language: English
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: gold
Estimated APC paid: $1,280
OpenAlex ID: W7234316620