Work

Critical Pore Sizes and Distinct Ionic–Metallic Bonding during Lithium, Sodium, and Potassium Filling of Nanoporous Carbon

Year: 2026
Type: article
Abstract: Nanopore filling is increasingly important as a universal mechanism for Li, Na, and K storage in a range of carbon anodes, including hard carbon, yet the mechanism remains unclear. Using defined pore features in zeolite-templated carbon (ZTC) nanopores, we find that metal–pore matching, rather than pore size alone, governs low-voltage, high-capacity storage. Li exhibits a two-regime filling mechanism in which ionic-carbon wall adsorption competes with metallic clustering, whereas K shows continuous filling with energy changes resembling a solid solution profile. In comparison, Na shows both mechanisms, depending on pore size. This metal-dependent filling chemistry enables alkali compositions beyond graphite intercalation limits, with Li approaching LiC1.2 compared with LiC6 and K reaching KC5.6 compared with KC8. This higher alkali content corresponds to predicted capacities that increase with pore size and fall within reported experimental ranges (e.g., ∼1600, 700, 400 mAh g–1 for Li, Na, and K, respectively, in ∼1.5 nm pores). However, extending the pore size toward the micropore/mesopore region does not necessarily increase useful capacity; instead, it promotes metallic regions that reduce the benefit of confined storage. Selected metal-pore combinations produce ∼0.1 V storage above the metal deposition voltage, consistent with the low-voltage plateau observed in Na-filled hard carbons. These results establish metal-specific pore topology as a design variable for optimizing hard carbon anodes beyond a one-size-fits-all pore-size strategy.
Source: ACS Nano
Institution: Brown University
Language: English
Open Access status: hybrid
Estimated APC paid: $4,500
OpenAlex ID: W7234588942
FWCI:
Cites: 45
Cited by:
Related to: 10