Effects of graphene nanoplatelets on early-age hydration and strength development of Na2CO3-activated ground granulated blast-furnace slag (GGBS) concrete
Year: 2026
Type: article
Abstract: Na₂CO₃-activated ground granulated blast-furnace slag (GGBS) concrete is a low-carbon alternative to Portland cement, but its delayed setting and low early-age strength limit its use. This study investigates how graphene nanoplatelets (GNPs, 0.005–0.02 wt% of GGBS) affect setting, hydration kinetics, microstructure, and strength. GNPs progressively shortened setting and advanced main gel precipitation peak from ~48 h (control) to ~24 h at 0.02% GNP, whereas cumulative heat converged after 72 h. XRD and TGA demonstrated calcite in reduced crystallinity/quantity and more advanced hydration at 3 days, with differences vanishing by 7 days, indicating that GNPs accelerate the reaction without changing its extent or phase assemblage. SEM/EDS revealed denser microstructures at intermediate GNP dosages and increasingly Ca-rich gels (Ca/Si from 1.33 to 2.59). At 0.01% GNP, compressive strength increased by 36% at 3 days and 41% at 7 days, whereas 0.02% GNP reduced the benefit through agglomeration-induced defects and poorer workability. A dosage of 0.0075–0.01% provided the best balance of strength, microstructural homogeneity, and workability.
Authors: Yongcong Zhao(Data curation, Formal analysis, Investigation, Writing – original draft), Gurkan Yildirim(Investigation, Validation, Writing – original draft), Yong Wang(Supervision, Writing – review & editing), Cise Unluer(Methodology, Writing – review & editing), Meini Su(Conceptualization, Funding acquisition, Methodology, Supervision, Writing – review & editing)
Language: English
Subfield: Civil and Structural Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: hybrid
Estimated APC paid: $4,540
OpenAlex ID: W7234883768