Work

Multi-scale and multi-technique characterization of a new ultra-fine ground glass pozzolan as a high content supplementary cementitious material

Year: 2026
Type: article
Abstract: The carbon intensity of cement production and the declining supply of conventional supplementary cementitious materials (SCMs), driven by the phasing out of coal-fired electricity and the transition to electric furnace steelmaking, necessitate the identification of viable alternative SCMs. Whereas ground glass pozzolan (GGP) has emerged as a promising candidate, most existing applications are limited to around 20% replacement of cement, with higher replacement levels adversely affecting the development of mechanical strength—predominantly controlled by GGP particle size, which can limit or enhance reactivity. Herein, a novel ultra-fine ground glass pozzolan ( uf -GGP) with a median particle size (D 50 ) of 4.16 µm—more than three times finer than conventional GGP (D 50 ≈ 15 µm)—is investigated as an SCM at cement replacement levels up to 50% by mass, extending well beyond the 20% range in the mainstream literature. A multi-technique characterization approach was implemented on: ( i ) cement mortars (compressive strength and electrical resistivity, considering both the standard ASTM mixing method and a high-shear mixing method) and (ii) pastes (microstructural characterization and analysis, including thermogravimetry, X-ray diffraction, scanning electron microscopy with energy-dispersive spectroscopy, and thermodynamic modelling). Results show that clinker-dilution-related early-age compressive strength losses in uf -GGP mortars are progressively recovered through pozzolanic reaction, with 20–40% cement replacement significantly exceeding the control (0% replacement) at 91 days under high-shear mixing, which was found to be critical at high uf -GGP contents, while under ASTM mixing the optimal range was limited to 20–30%. The best overall performance was achieved at 40% uf -GGP using high-shear mixing, combining a 91-day compressive strength about 8% above that of the control with an approximately 16 times increase in electrical resistivity, which increased further, up to 30 times that of the control, at 50% uf -GGP, consistent with a refinement of the pore structure. Thermodynamic modelling of uf -GGP pastes indicated an uf -GGP content threshold between 40% and 50% cement replacement, beyond which complete portlandite consumption is predicted to cause strätlingite formation, constraining C–S–H production and limiting further compressive strength development. A simplified environmental assessment showed that 50% uf -GGP reduced the embodied CO 2 of the mortar by 46%, despite the observation that the embodied energy decreased by only 7% due to the grinding energy needed to produce the ultra-fine powder. Overall, uf -GGP could allow cement replacement levels well beyond those currently achievable with conventional GGP, which should be confirmed at the concrete scale .
Institution: McMaster University
Language: English
Open Access status: hybrid
Estimated APC paid: $4,540
OpenAlex ID: W7234889112
FWCI:
Cites: 39
Cited by:
Related to: 10