High-Temperature Deformation Behavior and Hot Workability of a Ti2AlNb-Based Alloy

Year: 2026
Type: article
Abstract: Ti2AlNb-based alloys are promising candidates for aeroengine hot-section components, but their narrow processing windows complicate hot forming. This study investigates the flow behaviors and hot workability of a forged Ti2AlNb-based alloy using isothermal compression tests at deformation temperature of 970–1060 °C and strain rates of 0.01–10 s−1. Four constitutive models are established to describe the flow behaviors, including strain-compensated Arrhenius, multiple linear regression, standard backpropagation (BP), and sparrow-search-optimized BP (SSA-BP) models. The SSA-BP model achieves the highest prediction accuracy, with correlation coefficients of 0.998 and 0.995 for the training and testing sets, respectively. The corresponding mean absolute relative errors are 1.95% and 3.31%, and the root mean square errors are 4.36 and 7.49 MPa. Processing maps constructed based on the Murty instability criterion identify a preferred hot processing window of 1030–1060 °C and 0.01–0.5 s−1 across the evaluated strains. Electron backscatter diffraction reveals a lower α2 phase fraction and a modest increase in the recrystallized grain fraction at higher temperatures. Higher strain rates suppress recrystallization and limit the growth of recrystallized grains. These findings provide alloy-specific guidance for selecting hot processing parameters.
Source: Crystals
Language: English
Open Access status: gold
Estimated APC paid: $2,534
OpenAlex ID: W7234961884
FWCI:
Cites: 60
Cited by:
Related to: 10