Effect of Divalent Manganese Modification and Preparation Process on Lead-free Bismuth Ferrite Barium Titanate Piezoelectric Ceramics

Year: 2026
Type: dissertation
Abstract: Research on lead-free piezoelectric ceramics requires a balance between piezoelectric response and thermal stability. In the (1-x)BiFeO3-xBaTiO3 (BF–BT) system, BF helps maintain relatively high thermal stability, while BT promotes polarization switching and piezoelectric response. The coexistence of rhombohedral and pseudo-cubic phases gives 0.7BF-0.3BT an MPB and the potential to balance these two properties. However, Bi volatilization, phase stability, leakage, and defect chemistry make its properties rather sensitive to processing conditions. Mn modified 0.7Bi(Fe1-xMnx)O3-0.3BaTiO3 (0.7BFM-0.3BT) can affect charge compensation, carrier trapping, and domain wall motion, but its effect depends on the Mn precursor composition and heat treatment conditions. Compared to the existing work on Mn4+-doped 0.7BFM-0.3BT, the use of Mn2+ alone to modify 0.7BF-0.3BT has received limited attention. In this study, 0.7BFM-0.3BT ceramics containing 1 and 1.25 mol% Mn2+ were prepared using MnO as the precursor. The objective was to examine how Mn2+ modification and changes in processing affect the structure and properties of this system, and to find preparation conditions that offer a reasonable balance between piezoelectric and thermal properties. Most samples contained 2 mol% excess Bi2O3, and samples without excess Bi were also prepared as a control group. Undoped 0.7BF-0.3BT samples and 1 mol% Mn4+-doped 0.7BFM-0.3BT samples made with MnO2 as the precursor were prepared as controls for the Mn2+ system. Samples made by the conventional solid-state method were ball milled, calcined at 700 °C or 780 °C for 3h, pressed, and subjected to binder burnout before sintering at 930, 960, 990 or 1020 °C for 3h. Mn2+-doped samples prepared by the perovskite method were also compared with those made by the conventional solid-state method. Three poling methods were used and compared: DC, AC, and DC-biased AC poling. Characterization covered density, phase composition and microstructure by XRD and SEM/EDS, dielectric properties, piezoelectric coefficient, Curie temperature, and electromechanical coupling. The 1 mol% Mn2+ samples with 2 mol% excess Bi showed a fairly balanced set of properties after calcination at 700 °C for 3h, sintering at 960 °C for 3 h, and DC poling. The relative density was about 96.78%, and the relative permittivity and dielectric loss at room temperature and 100 kHz were about 513 and 0.078, respectively. The d33 at room temperature and 100Hz was 148 pC/N. The planar and thickness electromechanical coupling coefficients were 26.4% and 25.4%, respectively, with a Curie temperature of about 389 °C. The results show that the room-temperature permittivity and d33 of the Mn2+ system varied less across the sintering temperatures used than those of the undoped and Mn4+-doped systems. However, density, electromechanical coupling and Curie temperature fluctuated as the sintering temperature changed. Mn2+ modification improved the low-frequency dielectric loss at room temperature compared to the undoped system. For samples sintered at 990 °C under the same conditions, the Mn2+ system had a higher room-temperature permittivity at 100 kHz and lower loss than the Mn4+ system, along with slightly higher values of both electromechanical coupling coefficients. The conventional solid-state method combined with DC poling gave the Mn2+ system good overall properties with a reasonable balance among them. The choice of sintering conditions needs to take into account the different requirements for piezoelectric response, electromechanical coupling and Curie temperature.
Author: Wang, Yusen
Language: English
Open Access status: green
OpenAlex ID: W7235017198
Cites:
Cited by:
Related to: 10