Work

Full-range flexural modelling of hybrid-reinforced steel fibre recycled aggregate concrete beams

Year: 2026
Type: article
Abstract: Hybrid FRP-steel reinforcement and steel fibre-reinforced recycled aggregate concrete (SFRAC) can improve crack control and deformation capacity, but the full-range flexural response of hybrid SFRAC beams remains insufficiently quantified. This study developed a four-stage semi-analytical model for the load-mid-span deflection response of hybrid FRP-steel-reinforced SFRAC beams. Nine beams, comprising eight hybrid specimens and one all-steel reference, underwent four-point bending. Parameters included steel-fibre volume fraction, lower-to-upper bottom-reinforcement area ratio and lower-layer reinforcement type. A nonlinear finite-element model with explicitly embedded steel fibres interpreted pre-peak response, reinforcement-strain development, and damage distribution. The semi-analytical model defines cracking, yielding, ultimate, and post-peak reference states through sectional equilibrium, strain compatibility, an equivalent fibre-bridging force, ultimate-curvature correction, and calibrated post-peak secant stiffness. Compared with the identically reinforced fibre-free beam, steel-fibre volume fractions of 0.5%, 1.0%, 1.5%, and 2.0% increased the ultimate load by 8.9%, 12.6%, 13.6%, and 16.4%. Increasing lower-layer BFRP bar diameter from 10 to 14 and 18 mm increased ultimate load by 4.9% and 13.8%, respectively. Lower-layer BFRP and CFRP beams exceeded the all-steel reference’s ultimate load by 15.5% and 21.1%, respectively. Lower-layer FRP bars’ sustained elastic tensile contribution governed post-yield hardening. The fibre-bridging coefficient, ultimate-curvature coefficient, and post-peak secant stiffness were calibrated using five identically reinforced hybrid beams with steel-fibre volume fractions of 0–2.0% and held fixed thereafter. Internal assessment using three held-out hybrid specimens gave MAPE values of 3.7%, 10.5%, 10.4%, and 8.2% for \(P_{{{\text{cr}}}}\) , \(P_{{\text{u}}}\) , \(\delta_{{\text{u}}}\) , and \(\delta_{{\text{f}}}\) respectively. An external literature assessment gave a 7.3% MAPE for \(P_{{\text{u}}}\) . The all-steel reference specimen identified the applicability boundary, indicating that the model is intended for beams with linearly elastic FRP reinforcement in the lower layer of bottom reinforcement. Further independent validation is needed before the calibrated coefficients are generalised.
Language: English
Open Access status: gold
Estimated APC paid: $2,690
OpenAlex ID: W7235604448
FWCI:
Cites: 57
Cited by:
Related to: 10