Work

Sintering strategies govern grain and domain evolution for enhanced piezoelectric response in KNN-based lead-free ceramics

Year: 2026
Type: article
Abstract: Lead-free potassium sodium niobate (KNN)-based piezoceramics are highly sensitive to sintering conditions, yet the microstructural origin of this processing dependence remains unclear. Here, a fixed-composition 0.96K0.48Na0.52Nb0.96Sb0.04O3–0.04Bi0.5Na0.5ZrO3 (KNNS-BNZ) ceramic was used to isolate the effect of sintering thermal history by comparing conventional sintering (CS), prolonged conventional sintering (PCS), and two-step sintering (TSS). The piezoelectric coefficient (d33) varies markedly with thermal history: CS at 1120 °C for 2 h yields approximately 260 pC/N, extending the dwell to 16 h increases d33 to 426 pC/N, and TSS at 1200 °C for 10 min followed by 1100 °C for 7 h further increases d33 to 493 pC/N. Across these representative states, the mean grain size increases from 0.77 to 2.11 and 6.57 μm, accompanied by stronger diffraction-peak splitting, larger tetragonal distortion, and a transition from fragmented domains to extended stripe-domain configurations. Polarization measurements further reveal that the coarse-grained TSS specimen retains a larger fraction of the field-induced polarization after field removal, consistent with its more stable remanent state. These results establish a thermal-history-driven processing–structure–property relationship in which grain coarsening and domain reorganization are closely associated with enhanced polarization retention and macroscopic piezoelectric response. This processing–structure–property relationship provides a practical route for optimizing KNN-based ceramics at fixed composition.
Language: English
Open Access status: gold
Estimated APC paid: $2,372
OpenAlex ID: W7235836903
FWCI:
Cites: 38
Cited by:
Related to: 10