Roasting-Assisted Cobalt Extraction from Saprolite Nickel Laterite through Sulphuric Acid Leaching and Cyanex 272 Separation
Year: 2026
Type: article
Abstract: The increasing use of electric vehicles has driven demand for metals such as nickel and cobalt, which are primarily used in battery cathodes. Rising demand for battery metals drives the need for effective nickel and cobalt recovery. This study examines the upgrading of cobalt from nickel laterite ore from Morowali, Central Sulawesi, Indonesia. Laterite, common in tropical regions, is a major source of these metals. Cobalt in laterite mineral deposits is often chemically bound to iron, especially in saprolite-type ores with high magnesium content, making its extraction technically difficult. In the chemical process, magnesium oxide reacts more readily with sulphuric acid than cobalt and nickel oxides do, making the extraction process inefficient. In this study, the ore was mixed with carbon and sodium sulfate, compacted, and roasted at 700–900°C for 2 hours. The highest cobalt content (0.188 wt%) was achieved at 700°C with 5% coal, though it is likely trapped in silicates. A leaching process using 2 M H₂SO₄, followed by pH adjustment to 4.5 with NH₄OH, enabled selective precipitation of iron, achieving up to 94.27% iron removal. The selective extraction process using Cyanex 272 showed a tendency to extract cobalt. However, due to the stripping inefficiency, cobalt recovery in this study remains limited and could be further improved.
Source: Evergreen
DOI: 10.5109/7452635
Institution: University of Indonesia
Language: English
Subfield: Metals and Alloys
Field: Materials Science
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W7236095905