Work

Influence of Thermosetting Adhesive System and Bar Geometry on Shear and Flexural Performance of Steel-Reinforced Scots Pine Timber

Year: 2026
Type: article
Abstract: Steel reinforcement can improve timber stiffness and load-bearing capacity, but bond performance depends on the adhesive system and steel bar geometry. This study investigated steel-to-pine wood joints bonded with polyurethane (PUR), melamine–urea–formaldehyde (MUF), phenol–formaldehyde (PF), a PF/pMDI (polymeric methylene diphenyl diisocyanate) mixture modified with recycled rubber, and a polyester-based chemical anchor mortar (FIS). Pull-out and four-point bending tests were performed. For smooth bars, PUR achieved shear strengths of 2.81–2.86 MPa, compared with 0.46–0.53 MPa for MUF. For ribbed bars, MUF achieved 1.36–2.44 MPa, whereas PUR reached 0.37–1.10 MPa, depending on bar diameter. The PF/pMDI/rubber mixture achieved a mean shear strength of 3.14 MPa. In bending tests, the modulus of elasticity increased by approximately 30–50% compared with unreinforced pine for the PFP, PF, MUF, and FIS systems. Mean bending strength reached 63.5 MPa for the PF/pMDI/rubber (PFP) system and 71.2 MPa for MUF, while FIS achieved 71.1 MPa. No statistically significant differences were found among the PFP, MUF, and FIS systems. X-ray computed tomography revealed differences in adhesive distribution and void filling around the steel bars. The results indicate the potential of thermosetting adhesive systems for timber reinforcement, although further tests on structural-scale elements are required.
Source: Materials
Language: English
Open Access status: gold
Estimated APC paid: $3,137
OpenAlex ID: W7236237381
FWCI:
Cites:
Cited by:
Related to: 10