Work

Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments

Year: 2026
Type: article
Abstract: Fiber‐reinforced polymer (FRP) composites may undergo mechanical degradation in aggressive chemical environments, while concentration‐dependent differences between acidic and alkaline exposure remain insufficiently characterized for the same GFRP bar system. In this study, pultruded vinyl‐ester GFRP bars were exposed at room temperature to H 2 SO 4 and NaOH solutions with concentrations ranging from 0.5 to 3.0 mol/L for 30 and 60 days. Density, tensile strength, and shear strength were evaluated, while SEM, qualitative EDS, and FTIR were used to characterize local material changes. Under H 2 SO 4 exposure, tensile‐strength retention remained at or above 97.0%, whereas shear‐strength retention decreased to 92.6% after 60 days in 3.0 mol/L solution. Localized fiber‐surface roughening and gaps near some fiber/resin boundaries were observed. Under NaOH exposure, tensile‐strength retention decreased to 90.0% under the same concentration and duration, while shear‐strength retention remained at 98.4%. More evident surface‐resin loss and fiber exposure were observed, and the FTIR results were consistent with alteration of the vinyl‐ester matrix. Thus, the same GFRP bar system exhibited a greater relative reduction in shear strength under H 2 SO 4 exposure but a greater relative reduction in tensile strength under NaOH exposure. An empirical semi‐logarithmic relationship was used to compare the apparent degradation rates only within the measured 0–60‐day interval. These results highlight the value of jointly assessing tensile and shear retention when characterizing the short‐term chemical durability of GFRP bars.
Institution: Guizhou University
Language: English
Open Access status: bronze
OpenAlex ID: W7236442350
FWCI:
Cites: 49
Cited by:
Related to: 10