Effect of Longitudinal Reinforcement Configuration on ASR Surface Cracking at Nearly Constant Longitudinal Reinforcement Ratio
Year: 2026
Type: article
Abstract: This study examined how the arrangement of longitudinal reinforcement influences visible alkali–silica reaction (ASR)-associated cracking at nearly constant longitudinal steel ratio. Fourteen concrete cylinders (200 mm × 400 mm) were exposed under nominal 38 °C or 60 °C conditions for approximately 65 d. Each exposure series contained an unreinforced reference and two independently cast cylinders for each of three reinforcement layouts: 3-D20 (S1), 6-D14 (S2), and 12-D10 (S3). Mapped crack trajectories were evaluated in terms of length density, global longitudinal–transverse balance B, and local directional dispersion HQ*. At 38 °C, lateral crack-length-density ranges decreased from S1 (10.35–10.59 m/m2) to S2 (4.60–6.15 m/m2) and S3 (3.09–4.17 m/m2); the 60 °C ranges overlapped. Both unreinforced references were transversely/circumferentially biased, whereas all twelve reinforced cylinders were longitudinally biased. The B group means decreased from S1 to S3 at 38 °C and increased from S1 to S3 at 60 °C, with overlap among the 38 °C individual B values. At 60 °C, HQ* was lower in S3 than in S2 and S1 across the independent-specimen ranges. An embedded–surface comparison within the common 14-day observation window used the valid records from each channel to examine layout-associated differences in the timing of central and surface longitudinal deformation. The results show that redistributing a nearly constant amount of longitudinal steel changes both the amount and directional organization of visible cracking.
Source: Materials
DOI: 10.3390/ma19224891
Institution: Kobe University
Language: English
Subfield: Civil and Structural Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: gold
Estimated APC paid: $3,137
OpenAlex ID: W7236617833