Evaluation of plasticity and damage evolution of welded S355 steel and its heat-affected zone
Year: 2026
Type: article
Abstract: Welded joints are critical regions in steel structures where complex microstructures can reduce local ductility and fracture resistance. Stress triaxiality assessment is essential in welded joint analysis, as it enables the identification of highly constrained regions, such as the weld toe and heat-affected zone (HAZ), where crack initiation and propagation are more likely. These regions exhibit reduced ductility and an increased susceptibility to brittle failure, particularly in the presence of mechanisms such as hydrogen-induced cracking in offshore structures and pipelines. This study investigates the influence of stress triaxiality and microstructural heterogeneity on the plasticity and fracture behavior of S355 structural steel, its heat-affected zone (HAZ), and a representative weld metal. To investigate the material ductility and damage criteria for welded regions with potential difference in fracture strain, triaxiality stress-state, different notched specimens were tested to introduce controlled variations in triaxiality under different loading conditions. Local strain evolution and fracture strain were measured using Digital Image Correlation (DIC), while Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS) were employed to analyses fracture surfaces and identify microstructural and compositional features. The results reveal pronounced differences in fracture strain and triaxiality sensitivity between the base metal, HAZ, and weld metal. The HAZ exhibited the lowest ductility and the highest susceptibility to shear and mixed-mode loading, whereas the parent S355 steel retained higher strain and mixed-mode capacity. SEM observations confirmed that void nucleation and coalescence are highly different over welded regions, with less ductile fracture mechanics in the HAZ. The experimentally derived plasticity and fracture strain–triaxiality relationships were used to calibrate Bai–Wierzbicki (B–W) fracture loci, assessing strain capacity in welded structures. The findings are directly relevant to the plastic deformation regime and to structural scenarios involving low-cycle fatigue, accidental overload, and impact or collision events, where large strains and multiaxial cyclic stress states develop in welded zones. By quantifying the interplay between triaxiality, ductility, anisotropy, and microstructure, this work contributes to improved strain-based design and fracture assessment methods for critical welded steel structures.
Authors: Even Englund, R. M. Chandima Ratnayake
Institution: University of Stavanger
Language: English
Subfield: Mechanical Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: hybrid
Estimated APC paid: $3,990
Funder: Universitetet i Stavanger
OpenAlex ID: W7237130403