Interfacial Structure of Silane-Modified Hollow Silica Microspheres: Alkyl-Chain-Length Effects on Char Evolution and Ablation Resistance of Ethylene–Propylene–Diene Rubber Composites

Year: 2026
Type: preprint
Abstract: The polar surface of hollow silica microspheres (HSMs) is poorly compatible with nonpolar ethylene–propylene–diene rubber (EPDM), but its influence on residual-char evolution remains unclear. HSMs from the same batch were modified with trimethoxysilane, methyltrimethoxysilane, butyltrimethoxysilane, and octyltrimethoxysilane (OTMS) to distinguish the intrinsic protection of the hollow filler from the contribution of interfacial regulation. Interfacial measurements, molecular dynamics simulations, mechanical testing, and post-ablation characterization showed that increasing alkyl-chain length reduced surface polarity, strengthened filler–rubber association, and restricted EPDM chain mobility. These changes improved HSM dispersion and refined the pore architecture of the residual char. Compared with unmodified HSMs/EPDM, the OTMS-modified composite showed a decrease in accessible porosity from 22.9% to 17.5% and in the fraction of pore entries larger than 1000 nm from 68.2% to 39.1%, together with improved char continuity and mechanical integrity. Its mass and linear ablation rates were further reduced by 19.1% and 9.7%, respectively. These results connect pre-ablation interfacial chemistry with post-ablation pore structure and demonstrate that silane-chain-length regulation enhances the protective performance of HSM-filled EPDM composites.
Language: English
Open Access status: green
OpenAlex ID: W7238796087
Cites: 35
Cited by:
Related to: