Printing Orientation Affects Bond Strength and Thermal Shock Resistance of Digital Light Processing-Printed Zirconia-Veneer Systems
Year: 2026
Type: article
Abstract: Objectives To evaluate the effect of printing orientation on shear bond strength (SBS) and thermal shock resistance (TSR) of porcelain-veneered zirconia composites fabricated by digital light processing (DLP). Methods 3 mol% yttria-stabilised tetragonal zirconia polycrystal (3Y-TZP) specimens were manufactured via DLP at 0° (DLP0) and 90° (DLP90) orientations, with a milled group (CM) serving as the control. The coefficient of thermal expansion (CTE), surface topography, and grain orientation of the zirconia specimens were characterised. After surface grinding and veneering, the core-veneer assemblies underwent SBS testing (with/without prior thermocycling) and failure analyses. The TSR of the core-veneer crowns was also assessed. Data were statistically analysed (α = 0.05). Results DLP0 exhibited a significantly higher CTE than DLP90 ( P < .05). Ra and Rz were highest in DLP90, followed by CM and DLP0 ( P < .05). Initial SBS was comparable across groups ( P > .05), with means > 20 MPa. Following thermocycling, SBS significantly decreased in CM and DLP0 ( P < .05), whereas DLP90 maintained its bond strength ( P > .05), yielding a significantly higher post-ageing SBS (27.10 MPa, P < .05) than the other groups. Fractography revealed no adhesive failure in any group; veneering porcelain infiltrated the DLP90 interlayer gaps. CM core-veneer crowns achieved the highest TSR, significantly outperforming DLP0 ( P < .05). Conclusion The SBS and TSR of DLP-printed zirconia-veneer systems depend highly on printing orientation, which is associated with zirconia’s anisotropic CTE and surface features. Clinical relevance Although horizontal and vertical printing both provide clinically acceptable zirconia-veneer bond strength and thermal shock resistance, vertical printing further improves the interfacial resistance to thermal ageing and thermal stability of the bilayered crowns. Therefore, printing orientation is crucial for the long-term structural reliability of DLP-printed bilayered restorations.
Source: International Dental Journal
Institutions: Zhejiang Chinese Medical University, University of Hong Kong
Language: English
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: gold
Estimated APC paid: $2,550
OpenAlex ID: W7238815646