Abstract: The NH3-SCR performance of Fe-Ce-Mn/TiO2 catalysts depends on calcination temperature. To examine this effect at fixed composition, 8Fe2O3-5CeO2-40MnO2/TiO2 was prepared by co-precipitation and calcined at 200, 300, 400 or 500 °C for 4 h. The 400 °C sample provided the widest temperature range with at least 90% NO conversion (129–390 °C), reached a maximum of 99.17% and had the lowest apparent activation energy (55.78 kJ mol−1). It showed favorable N2 selectivity and retained the highest conversion in the SO2 and combined SO2/H2O resistance tests. XRD, N2 physisorption, microscopy, XPS, NH3-TPD and H2-TPR results showed that calcination altered pore development, particle aggregation and surface properties. At lower calcination temperatures, less developed pores and greater aggregation limited the exposure of supported metal species and coincided with poorer SCR performance. By 400 °C, pore development and particle dispersion had improved, accompanied by greater surface metal exposure, NH3 uptake and overall reducibility. Further heating to 500 °C increased aggregation and reduced surface metal fractions and total NH3 uptake without improving activity. Calcination at 400 °C for 4 h gave the best overall performance in the series.
Source: Catalysts
Language: English
Open Access status: gold
Estimated APC paid: $2,654
OpenAlex ID: W7238891657
FWCI:
Cites: 43
Cited by:
Related to: